Potters Choice glazes (AMACO writes it Potter's Choice, code PC) are the line most home potters mean when they say "AMACO glaze". They are mid-fire brushing glazes for cone 5 to 6 that copy the look of gas-kiln stoneware in an ordinary electric kiln. This review explains the cone range, the color families, the food safety labels and how the line behaves when layered.
It is research-based. We worked from AMACO's shop and product pages, its Complete Guide to Clay, Glazes and Underglazes, and US dealer listings. We have not fired these glazes, so descriptions of results are AMACO's.
Verdict
Potter's Choice is the easiest way to get gas-kiln surfaces from an electric kiln at cone 6. The range is wide, AMACO publishes layering combinations, and the glazes are sold in pints, so you can build a palette a jar at a time.
The trade-off is movement. Many colors are fluid by design, and AMACO itself warns about glaze flowing onto kiln shelves. Budget for test tiles, shelf protection and a learning curve. A pint typically costs about $20 to $40 at US sellers in October 2026, depending on color and seller; check the live price.
Potter's Choice specs at a glance
- Glaze fire: Cone 5, 2,167°F (1,186°C), to cone 6, 2,232°F (1,222°C), per AMACO
- Bisque: Cone 04, 1,945°F (1,063°C), per AMACO
- Atmosphere: Oxidation (electric kiln), sold as "reduction effects in oxidation"
- Colors: About 59 on AMACO's shop, coded PC-01 to PC-72 with gaps
- Sizes: Pint and gallon for most colors
- Coats: AMACO typically recommends 3 to 4 coats of its brushing glazes; its layering examples use 2 coats of Potter's Choice over 3 coats of Celadon
- Labels: AP or CL, and a Food Safe seal, shown color by color
- Companion lines: Potter's Choice Flux (PCF) and Dipping & Layering (DL)
Potter's Choice color families
AMACO groups the line loosely by effect. The table uses AMACO's own color names and, where we quote a look, AMACO's own words.
| Family | Example colors | What AMACO says | Notes |
|---|---|---|---|
| Floats | PC-23 Indigo Float, PC-24 Sapphire Float | Indigo Float: "intensely blue glaze with a lighter blue surface float" | Strong base colors for layering |
| Rutiles and flows | PC-20 Blue Rutile, PC-14 Lapis Flow, PC-21 Arctic Blue | Blue Rutile: "flowing light blue where thick and breaks brown where thinner" | Fluid; watch thickness |
| Flux | PC-17 Honey Flux | "Increases flow when layered over glazes" | Usually a top layer |
| Greens | PC-42 Seaweed, PC-44 Sage, PC-46 Lustrous Jade, PC-40 True Celadon | Seaweed: "fluid, deep green" that "breaks brownish over texture" | Seaweed runs when thick |
| Iron and earth tones | PC-30 Temmoku, PC-32 Albany Slip Brown, PC-33 Iron Lustre, PC-36 Ironstone | Named after traditional iron glazes | Common bases in AMACO combinations |
| Metallics | PC-01 Saturation Metallic, PC-02 Saturation Gold, PC-09 Vintage Gold | Saturation Metallic: "a satin metallic black glaze that resembles steel" | AMACO suggests it as an accent glaze |
| Speckles, aventurines, Cosmic | PC-29 Deep Olive Speckle, PC-64 Aventurine, PC-66 Cosmic Oilspot | See each product page | Effects vary with cooling and thickness |
| Reds | PC-59 Deep Firebrick, PC-70 Copper Red, PC-71 Flambe | See each product page | Test before committing a whole piece |
Can Potter's Choice be fired at cone 05?
No. AMACO formulates Potter's Choice for cone 5 to 6 and publishes no cone 05 results. Fired at cone 05, about 1,888°F (1,031°C), a mid-fire glaze will not melt fully, so you would get a dry, underfired surface instead of the floats and breaks shown on the jar. An underfired glaze is also not one you should treat as food safe.
If your kiln only reaches low fire, use AMACO's cone 05 lines instead: Teacher's Palette or LG Low Fire Gloss. Our AMACO glazes review lists every line by cone, and the pottery cone chart shows how far apart cone 05 and cone 6 really are.
Are Potter's Choice glazes food safe?
Many colors are, but you have to check each one. AMACO shows a Food Safe seal on qualifying product pages and in its Complete Guide, and says the seal "indicates that all FDA Guidelines for a food safe surface have been met". The seal belongs to the color, not to the whole line.
AMACO also notes that a glaze can be considered food safe yet "not recommended for use on food surfaces due to the durability of the glaze". And the AP or CL seal does not tell you anything about food use; AMACO says so directly.
A Food Safe seal describes one glaze fired correctly on its own. Layering two food-safe glazes makes a new glaze that nobody has tested on your clay. Fire to cone 5 to 6 as stated, keep fluid combinations off the inside of mugs until you have tested them, and see our food safe glaze guide for what testing involves.
Layering Potter's Choice
Layering is the main reason people buy this line. The usual pattern in AMACO's published combinations is a stiffer base glaze with a more fluid glaze on top, for example two coats of a Potter's Choice color over three coats of a Celadon. The top glaze melts into the base, and the two react where they meet.
Our AMACO glaze layering guide covers which glaze goes on top, thickness and drip control, and lists combinations AMACO has published by name. Two popular top layers have their own pages: Honey Flux combinations and Seaweed combinations.
Pints vs dry dipping mixes
Brushing pints are the standard format. Several colors are also sold as dry dipping mixes, which you mix with water yourself. AMACO warns that "all dry dipping glazes can be difficult to layer" and that "dipping glazes behave differently from brushing", so a combination that works with pints may not match with a dipping bucket. Mixing dry glaze also means handling silica powder: wear a NIOSH-approved respirator and see our guide to mixing glaze from powder.
Building a first Potter's Choice palette
Four jars are enough to learn the line: one dark base, one fluid top glaze, one flux and one color you simply like. That gives you each glaze alone plus several pairings to test. The four colors below cover those roles using AMACO's own descriptions. Add a Celadon if you want a transparent base, since AMACO uses Celadons under Potter's Choice in its examples.
PC-20 Blue Rutile
AMACO says Blue Rutile is "always one of our top selling Potters Choice glazes". It flows light blue where thick and breaks brown where thin, which makes it a strong texture glaze and a frequent partner in layering.
- Finish: Opaque, fluid
- Sizes: Pint, gallon
- Label: AP shown on AMACO's page
Pros
- Classic Potter's Choice look
- Shows texture
- Layers widely
Cons
- AMACO calls it "a very fluid glaze"
- Thickness changes the color a lot
Who should skip it: Potters who want a flat, even blue.
PC-23 Indigo Float
Indigo Float is "an intensely blue glaze with a lighter blue surface float" that "breaks deep blue where thinner". A dark, rich cobalt base gives the more fluid colors something to contrast against, which is why it shows up in so many layered pots.
- Finish: Opaque
- Sizes: Pint, gallon
- Label: AP shown on AMACO's page
Pros
- Deep cobalt color
- Good base for layering
- Float effect on its own
Cons
- Dark, so it hides fine carving
- Dry dipping version needs separate testing
Who should skip it: Anyone after light, pastel surfaces.
PC-17 Honey Flux
AMACO describes Honey Flux as "a creamy color that increases flow when layered over glazes", opaque honey and cream at cone 5, shifting to "a beautiful fluid white with honey flecks at Cone 6". It is a layering tool more than a stand-alone glaze.
- Finish: Opaque
- Sizes: Pint, gallon
- Label: AP/CL marks shown; AMACO marks it not for spraying
Pros
- Adds movement to almost any base
- Visible change between cone 5 and cone 6
Cons
- Extra flow means extra drip risk
- Not for spraying
Who should skip it: Beginners not yet using a catch tray or cookie.
PC-42 Seaweed
Seaweed is "a fluid, deep green glaze that layers beautifully with a variety of Potter's Choice glazes", breaking brownish over texture. AMACO adds a clear warning: "Pay attention to application thickness so the glaze does not flow onto kiln shelves during firing."
- Finish: Opaque, fluid
- Sizes: Pint, gallon
- Food Safe seal: check the current product page
Pros
- Rich green
- Breaks over texture
- Layers with many colors
Cons
- Runs when thick, per AMACO
- Needs shelf protection
Who should skip it: Anyone glazing to the foot of a pot without a cookie.
What Potter's Choice does well
- Gas-style surfaces from an electric kiln at cone 5 to 6.
- A deep catalog of named layering combinations from AMACO.
- Pint sizes make it cheap to try one new color at a time.
- Clear per-color marks for cone, opacity, spraying and food safety.
Weak points
- Many colors move; shelf drips are the most common complaint with fluid glazes.
- AMACO recommends firing test tiles "before using each new batch number of glaze".
- Results depend on thickness, clay body and cooling, so photos are only a starting point.
- Brushing three or more coats is slow for production work.
Who should buy it, and who should skip it
Buy Potter's Choice if you fire an electric kiln to cone 5 or 6, enjoy experimenting, and are ready to make test tiles. It suits mugs, bowls and vases with texture where a breaking glaze has something to show off.
Skip it if you fire to cone 05, if you want flat, predictable color for production ware, or if you cannot protect your shelves. Satin Matte or a dipping clear is easier for plain functional work.
Alternatives
- AMACO Celadon: transparent, mixable color that pools in texture and is a common Potter's Choice base.
- Mayco Stoneware glazes: Mayco's mid-fire line; compare the brands in AMACO vs Mayco.
- Spectrum glazes: another mid-fire brand with layering combinations.
Sources: AMACO shop line page for Potter's Choice (three pages of colors); AMACO product pages for PC-01 Saturation Metallic, PC-17 Honey Flux, PC-20 Blue Rutile, PC-23 Indigo Float and PC-42 Seaweed; AMACO Complete Guide to Clay, Glazes and Underglazes (amaco.com). Research-based, not hands-on. Specs checked October 2026.