Verdict: a reliable default, with known weak colors
AMACO Velvet underglaze is the line we would point a new home potter to first. AMACO rates it from cone 05 to cone 10, says it can go on wet, leather-hard or bone-dry greenware or on bisque, and gives it a food-safety status under three of its own clear glazes. Very few underglazes cover that much ground in one jar. The weak spot is the top of the range: AMACO itself says some pigments may burn out at higher temperatures, and dealer notes show which colors shift most.
This review is research-based. We did not fire Velvet ourselves; we compared AMACO's product sheet and shop pages with dealer listings at Blick, Clay-King, Krueger Pottery and The Ceramic Shop, and we flag where they disagree. Specs checked October 2026.
AMACO Velvet specs
| Spec | AMACO Velvet Underglaze | Source |
|---|---|---|
| Cone range | 05 to 10; most vibrant 05 to 5 | AMACO product sheet (Blick lists 06 to 10) |
| Clay stage | Wet, leather-hard or bone-dry greenware; mature cone 04 bisque | AMACO |
| Coats for opaque color | 3 | Blick, Clay-King |
| Finish unglazed | Velvety smooth, matte; stiff, will not run | AMACO |
| Under clear glaze | More saturated color | AMACO |
| Food-safety status | Approved when fired under AMACO LG-10, F-10 or HF-9 clear | AMACO |
| Sizes | 2 oz, 16 oz; some colors in gallons | AMACO |
| Colors | Krueger lists 57 Velvet items; AMACO's shop shows 40+ | Krueger, AMACO shop |
| Safety labeling | Conforms to ASTM D-4236 | AMACO |
What AMACO Velvet does well
One jar for low fire and mid fire
The cone 05 to 10 rating is the main reason to buy Velvet. If you start on a small 120V kiln at cone 05 and later move to cone 6 stoneware, you keep your colors. AMACO says Velvet fires true to the wet color, which makes it easier to plan a design than glazes that look nothing like their fired result.
Every clay stage
AMACO lists wet clay, leather-hard and bone-dry greenware, and bisque. Decorating at leather hard suits sgraffito and mishima; decorating bisque is easier for beginners because the pot is stronger. Our pages on leather hard clay and bisque firing explain each stage.
Can you use Velvet underglaze on bisque?
Yes. AMACO lists mature cone 04 bisque, which it gives as 1,945°F (1,063°C), as a surface for Velvet, and dealer listings such as MC Art Supplies repeat "apply to wet clay, greenware or bisque." Bisque is the easier stage for many beginners because the pot is strong enough to handle while you paint. Wipe the bisque with a barely damp sponge to remove dust, build three coats, and let them dry before glazing. Because unfired Velvet can smear, sponge, dip, pour or spray the first coat of clear glaze rather than brushing it hard.
It stays put
AMACO describes Velvet as stiff, so it does not run in the kiln. That is what you want for crisp edges, lettering and carved lines. AMACO lists painting, sgraffito, mishima, screen printing, stamping and wax resist as uses, plus layering with its Opalescent glazes.
Easy to find
Velvet is stocked by most US pottery dealers, big craft chains and Amazon, as singles, pints and numbered sets. Dealer pricing for 2 oz jars ran roughly $8 to $12 in October 2026; check the live price.
More than one way to apply it
Krueger and The Ceramic Shop describe Velvet as sprayable, and AMACO also sells a separate Velvet Sprayz line for spray application. Thinned with water, Velvet works for washes; at full strength it holds a crisp edge for stencils, wax resist and screen printing. That range is useful once you move past simple brushwork.
Velvet with clear glaze
AMACO names three clear glazes for Velvet's food-safety status: LG-10 and F-10 for low fire, and HF-9 for mid fire. Lakeside Pottery's sgraffito tutorial and Elan Transfers both use HF-9 at cone 5 to 6, which makes it the common pairing for home stoneware. If you already have a favorite clear from another maker, Velvet will usually still look good under it, but AMACO's food-safety statement no longer covers that combination.
Apply the clear gently. A thick, brushed coat can drag unfired underglaze and blur lines, so many potters dip, pour or spray, or sponge the first coat. Our clear glaze for pottery guide compares clears by cone, and how to glaze pottery covers dipping and pouring.
Velvet on different clay bodies
Velvet colors look truest on white clay. AMACO's own No. 38 White Stoneware is rated cone 5 to 10 and fires white in oxidation, so it keeps underglaze colors clean, while buff bodies like AMACO No. 46 mute bright colors. On red or brown clay, paint a base of V-360 White first, or accept a darker, earthier result. Our stoneware clay guide lists white-firing options.
Reading the AMACO Velvet underglaze chart
AMACO publishes a Velvet color chart fired at cone 05, cone 5 and cone 10, and Blick links it from its Velvet listing. Dealer descriptions follow the same three cones. The table below collects what they say for a handful of popular colors so you can see the pattern: some colors deepen as you fire hotter, and some fade.
| Color | Cone 05 | Cone 5 | Cone 10 | Source |
|---|---|---|---|---|
| V-308 Yellow | Bright lemon, vivid | Still bright, less saturated | Pale | Krueger |
| V-318 Rose | Deep magenta | Patchy | Nearly burned out | Clay-King |
| V-321 Lilac | Light, soft plum | Warmer and deeper | Begins to burn out | The Ceramic Shop |
| V-329 Sea Glass | Very pale blue-green | About the same | More blue | Krueger |
| V-345 Light Green | Bright | Darkens to forest green | Deep pine green | Krueger |
| V-382 Red | Vivid crimson | Dark wine red | Brownish, begins to burn out | Krueger, Clay-King |
| V-388 Radiant Red | Bright scarlet | Deepens | Deep fire-engine red, slightly glossy | Krueger |
Research note: AMACO's chart and the dealer notes are fired at cone 5, not cone 6. Cone 6 is about 65°F hotter on Orton's chart (2,232°F (1,222°C) against 2,167°F (1,186°C) for self-supporting cones at 108°F per hour), so expect a color that is already shifting at cone 5 to shift a little more at cone 6. Fire a test tile before a big project.
If you want reds that hold at stoneware temperatures, the dealer notes point to V-388 Radiant Red rather than V-382 Red. Rose and other pinks are the riskiest choices for cone 6 work.
Weak points
- Three coats for solid color. Blick and Clay-King both give three coats for opaque coverage. On a big platter that is real time, and thin spots show after firing.
- Some colors fade hot. AMACO says some pigments may burn out at higher temperatures, and the chart above shows which ones dealers flag.
- Cone rating differs by source. AMACO's sheet says cone 05 to 10; Blick's listing says cone 06 to 10. The difference only matters if you fire below cone 05.
- Food use depends on the clear. AMACO's food-safety status is tied to LG-10, F-10 or HF-9. If you use another clear glaze, you are relying on that glaze maker and your own testing.
Pros
- Cone 05 to 10 rating
- Works on wet clay, greenware and bisque
- Stays crisp in firing
- Easy to buy in singles, pints and sets
Cons
- Three coats for opacity
- Pinks, rose and some reds fade at cone 10
- Food-safety status tied to specific AMACO clears
AMACO Velvet underglaze sets
AMACO sells Velvet as numbered sets of 2 oz jars, and Set 1 through Set 4 all appear at US dealers and on Amazon. Our product table lists the 12-color Set 4 on Amazon. Each set has a different color mix, so compare the color list against the chart above before you buy if you fire at cone 6 or higher. Blick also lists classroom packs. A set is the cheapest way to try the line; after that, buy your most-used colors in 16 oz jars.
A practical first palette for cone 6 potters is a black, a white, a blue, a green and one warm color that the dealer notes say holds its color, such as V-388 Radiant Red. Black and white do the most work: black for line drawing and sgraffito, white for base coats and for mixing pastels, since Velvet colors can be mixed with each other.
Can you mix AMACO Velvet underglazes?
Yes, within the Velvet line. Dealer listings describe Velvet colors as intermixable, and adding V-360 White to a color is the simplest way to make a pastel shade. The AMACO pages we checked do not publish mixing ratios or fired results for blends, so treat every mix as a new color: measure by spoonful or by weight, write the ratio on the jar, and fire a test tile at your cone before you use it on a finished piece. Pinks, reds and yellows can shift at cone 5 and above, so a blend that leans on one of them may shift too. Mixing Velvet with another brand's underglaze is possible but untested by either maker, which makes a test tile even more important.
How to apply Velvet for full color
- Make sure the surface is clean and free of dust and oils. On bisque, wipe with a barely damp sponge and let it dry.
- Stir the jar well. If it has thickened, add a few drops of water.
- Brush on the first coat with a soft brush. Let it lose its shine.
- Add the second and third coats, changing brush direction each time.
- Bisque fire if you decorated greenware, then apply clear glaze if you want gloss or a food surface.
For washes and watercolor effects, thin Velvet with water and use one coat. For sgraffito, build three coats at leather hard and carve when the underglaze has dried to a matte look.
Is Velvet good for beginners?
Yes, for three reasons that come straight from the specs. First, it forgives timing: you can paint wet clay, leather-hard or bone-dry greenware, or bisque, so a missed window is not a lost piece. Second, it fires close to the wet color, so what you paint is roughly what you get. Third, it does not run, so a beginner's uneven glaze firing will not smear the design. The one habit to build early is patience with coats: three even coats, each dried to matte, give the solid color the jar promises.
Who should buy AMACO Velvet, and who should skip it
Buy it if you fire anywhere from cone 05 to cone 6, want one line that works on greenware and bisque, and like a matte surface on decorative pieces with the option of clear glaze on functional ones.
Who should skip it: potters who fire cone 10 and want bright pinks or yellows, who may do better with a line formulated for high fire such as Coyote, and potters who only want line work, for whom an underglaze pencil is simpler.
Alternatives to AMACO Velvet
- AMACO LUG: AMACO's liquid underglaze, made to cover large areas quickly and listed for sgraffito and mishima. See our LUG review.
- Mayco Fundamentals: 50+ colors, cone 06 to 10, with a fired guide at cone 06, 6 and 10. See our Mayco Fundamentals page.
- Mayco Stroke & Coat: a glaze that brushes like an underglaze. Compare them in Velvet vs Stroke & Coat.
- The full shortlist: our best underglazes guide compares seven options side by side.
For the rest of AMACO's range, including clear glazes like HF-9, see our AMACO glazes overview.
Sources: AMACO Velvet product sheets (amaco.com assets) and AMACO shop Velvet page; Blick AMACO Velvet listing (cone range, coats, cone 05/5/10 chart PDFs); Clay-King listings for V-318 Rose and V-382 Red; Krueger Pottery listings for V-308, V-329, V-345, V-382 and V-388 and the Velvet collection; The Ceramic Shop listing for V-321 Lilac; MC Art Supplies AMACO Velvet listing (cone 05 to 10, wet clay, greenware or bisque, sprayable); Orton cone temperature chart. Specs checked October 2026.