L&L kilns come from L&L Kiln Mfg in Swedesboro, New Jersey, which says it was established in 1946 and calls itself the oldest consumer and school kiln maker in the US. The short answer for home potters: the Easy-Fire series is the line to shop, the e18S-3 is the sensible first kiln on 240V, and every Easy-Fire uses hard ceramic element holders, the feature L&L is best known for. For 120V homes, the small Plug-n-Fire reaches cone 10.
This review is research-based. We used L&L's own model pages, series pages and feature pages, and we did not fire these kilns. L&L kilns were not found on amazon.com in our research, so the product buttons here run an Amazon search; most buyers order through an L&L distributor.
Verdict: should you buy an L&L kiln?
If you want a kiln that is easier to maintain over many years, L&L makes a strong case. The element holders, 3 inch K23 brick on the Easy-Fire line, two thermocouples and a multi-zone Genesis touchscreen come standard rather than as upgrades.
The trade-offs are price, lead time and buying route. L&L lists MSRPs above some rivals of similar size, quotes 10 to 12 weeks for many models, and sells through distributors. If you need a kiln next week, this is not the brand.
L&L kiln specs by model
| Model | Electrical (240V 1-phase unless noted) | Fuse or breaker | Plug (NEMA) | Max temp | Interior | Price |
|---|---|---|---|---|---|---|
| Easy-Fire e18S-3 | 23.9A, 5,740 W (208V: 4,980 W) | 30A, 10 AWG | 6-50 cord | Cone 10, 2,350°F (1,288°C) | 16.5 in wide, 18 in high, 2.5 cu ft | Search Amazon |
| Easy-Fire e23T-3 | 48A, 11,520 W (208V: 9,978 W) | 60A, 6 gauge | 6-50 cord | Cone 10, 2,350°F (1,288°C) | 22.3 in wide, 27 in high, 6.7 cu ft | Search Amazon |
| Easy-Fire e23T-3, 3-phase | 27.7A at 240V, 11,520 W | 40A | 15-50 cord | Cone 10 | Same as above | Not for homes |
| Plug-n-Fire | 120V, 12.5A draw, 1,500 W | Standard 15A circuit | Not listed on page | Cone 10, 2,350°F (1,288°C) | 8 x 8 x 9 in, 0.33 cu ft | Search Amazon |
| DLH11-D | 120V, 18A, 2,160 W | 25A fuse (L&L page) | 5-20 | Cone 6, 2,230°F (1,221°C) | 11 in wide, 9 in high, 0.5 cu ft | Search Amazon |
| DL11-D | 120V, 1,847 W | 20A (series page) | Not listed | Cone 5, 2,170°F (1,188°C) | 0.5 cu ft | Dealer order |
Research notes: L&L's Easy-Fire series table calls the e18S-3 "18 inch" with an 18 inch diameter, while the e18S-3 model page gives a 16.5 inch interior diameter; we used the model page. The series table's amp column (for example 30 for the e18S-3) matches the fuse size on the model page rather than the 23.9A draw. The DLH11-D page lists a 25A fuse with a NEMA 5-20 plug, an unusual pairing; ask L&L or your electrician which breaker to use.
These are L&L's stated figures. A licensed electrician should size the breaker, wire and receptacle from the kiln's nameplate, your panel and local code. Do not wire a kiln circuit yourself.
What are L&L element holders?
In most electric kilns the coiled elements sit in grooves cut into soft firebrick, held at the corners with metal pins. L&L instead fits hard ceramic channels into the brick walls, and the elements sit in those channels. L&L's feature page says this means no pins, no loose brick crumbs falling into the kiln, and no damaged brick when you change elements.
L&L also claims the dense holder walls reflect heat, so elements run cooler relative to the chamber and last longer because they do not snag, bunch up and burn out. It says you can change elements without unstacking the kiln. We could not verify the element life claim with independent data, but the brick protection point is easy to see: pins and soft brick are the classic wear spot on older kilns. See our kiln elements guide for signs that elements need replacing.
L&L Easy-Fire e18S-3: the home studio pick
The e18S-3 is the Easy-Fire that fits a typical garage studio. L&L lists 240V single-phase at 23.9A and 5,740 W on a 30A fuse with 10 AWG wire, and it comes with a NEMA 6-50 cord. That 30A circuit is lighter than the 40A circuit many 18 inch rivals need, which can lower installation cost.
Inside it measures 16.5 inches across and 18 inches high, 2.5 cubic feet, with 3 inch K23 firebrick. It reaches cone 10, 2,350°F (1,288°C). The Genesis multi-zone touchscreen reads two thermocouples to even out temperature between the top and bottom, and the kiln weighs 185 lb.
- Electrical: 240V 1-phase, 23.9A, 5,740 W; 208V 1-phase, 23.9A, 4,980 W
- Fuse and wire: 30A, 10 AWG; NEMA 6-50 cord
- Max temperature: Cone 10, 2,350°F (1,288°C)
- Interior: 16.5 in diameter x 18 in high, 2.5 cu ft
- Brick: 3 in K23
- Controller: Genesis multi-zone touchscreen, two thermocouples
- Lead time: 10 to 12 weeks per L&L
- Price band: typically $3,300 to $3,700 before freight in October 2026, based on L&L's MSRP; check with a distributor
Pros
- Hard ceramic element holders
- 30A circuit for a cone 10 kiln
- Multi-zone control as standard
Cons
- Higher price than similar-size rivals
- Long lead time
- Smaller than its "18" name suggests
Who should skip it: Buyers on a tight budget or anyone who needs a kiln within a few weeks.
Our Easy-Fire review compares all ten Easy-Fire sizes.
L&L Easy-Fire e23T-3: big and tall
The e23T-3 is the large Easy-Fire many teaching studios use. L&L lists 6.7 cubic feet in a 22.3 inch by 27 inch chamber, cone 10, 3 inch K23 brick and 320 lb. On 240V single-phase it draws 48A and 11,520 W on a 60A fuse with 6 gauge wire and a NEMA 6-50 cord. A 3-phase version draws 27.7A on a 40A fuse with a NEMA 15-50 cord, and that version is not for normal single-phase homes.
Pros
- 6.7 cu ft
- Cone 10
- Element holders and multi-zone control
Cons
- 60A circuit
- Heavy
- 27 inch depth is a long reach for loading
Who should skip it: Hobby potters who fire small loads; the e18S-3 or a mid-height model fits better.
Which L&L kiln runs on 120V?
None of the Easy-Fire kilns run on 120V; L&L lists them at 240V or 208V. The 120V models are in L&L's craft and test kiln series.
Plug-n-Fire
L&L says the Plug-n-Fire fires to cone 10, 2,350°F (1,290°C on L&L's page), on most standard 15A circuits. It draws 12.5A and 1,500 W at 120V, has an 8 x 8 x 9 inch chamber (0.33 cubic feet), 2.5 inch K23 side walls with 1 inch backup insulation, a door safety switch that cuts power when opened, a Genesis Mini touchscreen, and a 3-year limited warranty. It weighs 77 lb and comes with one shelf and three posts.
Pros
- Cone 10 on a standard 15A circuit
- Door safety switch
- Shelf and posts included
Cons
- Very small chamber
- 8 to 10 week lead time
Who should skip it: Wheel throwers who want to fire more than a few small pieces at a time.
DLH11-D and DL11-D
The DLH11-D runs on 120V at 18A and 2,160 W with a NEMA 5-20 plug and reaches cone 6, 2,230°F (1,221°C). Its 11 inch by 9 inch chamber holds 0.5 cubic feet, it uses 2.5 inch K23 brick and hard ceramic element holders, and it weighs 95 lb. The DL11-D is the same size at 1,847 W but stops at cone 5. L&L warns that its 120V kilns are not meant for high production: firing to maximum temperature more than once a week shortens element life to a point L&L calls unacceptable.
Pros
- Cone 6 on 120V
- Element holders
- Wi-Fi Genesis Mini controller
Cons
- Needs a 20A-class circuit
- L&
- L advises against weekly max-temperature firing
Who should skip it: Anyone planning to fire to cone 6 every week; a 240V Easy-Fire will last longer.
Why do potters like L&L kilns?
Three reasons come up across L&L's own material and our spec comparison. First, the hard ceramic element holders protect soft brick and make element changes simpler. Second, Easy-Fire kilns come standard with 3 inch K23 brick, two thermocouples and a multi-zone touchscreen, features that are extra-cost upgrades on some other brands. Third, L&L publishes fuse, wire gauge and cord type for every voltage, which helps your electrician.
Our Skutt vs L&L comparison looks at how this plays out against the most common alternative.
How to choose L&L kiln size
Choose size from three things: how much you make between firings, your tallest piece, and the circuit you can add. L&L's own numbers show the jump between sizes. The e18S-3 holds 2.5 cubic feet in a 16.5 inch wide, 18 inch high chamber on a 30A fuse, while the e23T-3 holds 6.7 cubic feet, 22.3 inches wide and 27 inches high, but needs a 60A fuse. The 120V Plug-n-Fire holds 0.33 cubic feet and the DLH11-D 0.5 cubic feet.
- Tests, tiles and jewelry: Plug-n-Fire or DLH11-D on 120V. L&L warns that firing its 120V kilns to maximum more than once a week wears elements fast.
- Weekly mugs, bowls and small vases: e18S-3, which runs on a 30A circuit.
- Tall pieces, classes or sales stock: a taller or wider Easy-Fire such as the e23T-3, if your panel can take a 60A circuit.
Measure your tallest planned piece, then allow for shelves and posts above and below it. A kiln you fill every week or two is a better fit than a bigger one you fire half empty. Our kiln loading guide and 120V vs 240V guide help with the last two checks, and our Easy-Fire review lists all ten Easy-Fire sizes.
Where to buy L&L kilns: US dealers
L&L sells through authorized distributors rather than Amazon. Its distributor page says buying from one gets you "expert product advice, genuine L&L components, and full warranty support." US distributors listed in October 2026 include Sheffield Pottery (Massachusetts), Clay-King (South Carolina), The Ceramic Shop (Pennsylvania), Neil Estrick Gallery (Illinois), Clayworks Supply (Maryland), Rocky Mountain Clay (Colorado), Clay Planet (California) and Bracker's Good Earth Clays (Kansas). Use the locator on hotkilns.com to find the nearest one.
A nearby dealer helps with freight delivery, element and thermocouple parts, and service later. Ask about lead time, since L&L quotes 10 to 12 weeks for many Easy-Fire models and 8 to 10 weeks for the Plug-n-Fire, and ask whether a furniture kit and vent can ship on the same order. L&L's warranty, as hosted by The Ceramic Shop, runs three years from the original purchase and covers defective parts but not labor, with elements and thermocouples pro-rated. For used L&L kilns, see our kiln for sale guide.
Weak points
L&L costs more than many rivals of the same size, and its 10 to 12 week lead times are long. It is dealer-only in our research. The e18S-3 is smaller inside (16.5 inch diameter) than its name suggests. The largest Easy-Fire, the e28T-3, is rated to cone 8, 2,280°F, not cone 10, so check that if you plan to buy big.
Who should buy an L&L kiln, and who should skip
Buy an L&L if you plan to keep the kiln for a long time, care about maintenance, and want multi-zone control as standard. The e18S-3 suits most home potters on 240V, and the Plug-n-Fire suits a 120V home doing tests and small work. Skip L&L if price or delivery time decides your purchase, or if you want to buy on Amazon.
Follow L&L's clearance and ventilation instructions, keep combustibles away from the kiln, and never leave a firing unchecked against the manual's advice. Clean clay dust wet because it contains silica.
Alternatives to L&L
- Skutt kilns: wider dealer stock and Amazon listings.
- Paragon kilns: the Caldera is the main 120V cone 10 rival to the Plug-n-Fire.
- Olympic kilns: 3 inch brick Medallion models with lower list prices.
- Best kilns for home pottery: cross-brand picks.
Sources: L&L Kiln Mfg homepage and about page; L&L Easy-Fire series page; L&L model pages for e18S-3, e23T-3, Plug-n-Fire and DLH11-D; L&L craft and test kiln series page; L&L element holder feature page; L&L distributor page and kiln selector; The Ceramic Shop's copy of the L&L warranty. Specs checked October 2026.