Comparison

Stoneware vs Porcelain: Clay Bodies, Cones and Absorption Compared

Quick answer

Stoneware vs porcelain comes down to handling and color. Both fire at cone 5 to 6 or cone 10 and both can be dense enough for mugs and plates. Porcelain is whiter, finer and can be translucent, but it is softer on the wheel and warps more. Stoneware is cream, buff, gray or brown, more forgiving and usually cheaper. Pick the clay rated for your kiln's cone first, then choose by look and skill.

On this page
  1. Stoneware vs porcelain at a glance
  2. What each clay is made of
  3. Firing range: both come in cone 6 and cone 10
  4. Absorption and vitrification: what the data sheets say
  5. Shrinkage, warping and drying
  6. On the wheel and at the table: how they handle
  7. Color, glazes and translucency
  8. Strength, chips and everyday use
  9. Cost and buying
  10. Can you use both in one studio?
  11. Choose stoneware or porcelain
  12. What you need
  13. Frequently asked questions

Stoneware vs porcelain is not a choice between a weak clay and a strong one. Both are high-temperature clay bodies that US makers sell for cone 5 to 6 electric kilns and for cone 10, and both can fire dense and tight. The differences are what they are made of, how they feel on the wheel, how much they move in the kiln and how your glazes look. Stoneware is the forgiving everyday clay; porcelain is the white, fine, demanding one.

This comparison is research-based. We did not throw or fire these clays: we compared the makers' own data sheets and product pages from Laguna, Standard Clay, AMACO, Aardvark and Archie Bray. For the single clays in depth, see our stoneware clay and porcelain clay guides. Specs checked November 2026.

Stoneware vs porcelain at a glance

FeatureStonewarePorcelain
Main ingredientsBall clays and fire clays with feldspar and silica; often sand or grogKaolin (often grolleg) with feldspar and silica; little or no ball clay
Cones sold forCone 5 to 6 and cone 10; some list cone 5 to 10Cone 5 to 6 and cone 8 to 10
Fired colorCream, buff, gray, brown, red or blackWhite to gray-white; some creamy white
Absorption at the right cone (maker figures)About 0% to 3%About 0% to 2%, most under 1%
Shrinkage, wet to fired (maker figures)About 11% to 15%About 11% to 14%
TranslucencyNoYes when thin, for bodies made for it
On the wheelHolds shape, takes water, forgivingSoft, slick, collapses with too much water
Warping riskLowerHigher, especially wide flat forms
Best forLearning, everyday ware, large forms, plantersBright glazes, thin and light-catching pieces, fine detail

The ranges come from the bodies in the data table below.

What each clay is made of

Stoneware is built around plastic secondary clays such as ball clay and fire clay, which carry some iron and other minerals. That is why it fires cream to brown and why it throws so easily. Makers add feldspar to melt the body together and silica for glaze fit, and many add sand or grog for texture and strength.

Porcelain is built around kaolin, a purer white clay that is less plastic. Feldspar does more of the work, so a lot of the body turns to glass in the firing. Standard Clay says its 365 and 257 Grolleg Porcelains contain no ball clay, which keeps them white but makes them less plastic on the wheel. More plastic porcelains, such as Laguna's #16, which Laguna calls very plastic, trade a little whiteness for easier throwing.

Firing range: both come in cone 6 and cone 10

A common belief is that porcelain always needs a hotter kiln. It used to, but US makers now sell plenty of mid-fire porcelain for home electric kilns. The cone on the box matters far more than the word stoneware or porcelain.

  • Cone 5 to 6 stoneware: Laguna B-Mix 5 (WC401), AMACO No. 46 Buff (best at cone 5), AMACO No. 16 White Chocolate, Standard 182 Angel White (cone 6 to 10), Aardvark Bee Mix 5 and SBF.
  • Cone 5 to 6 porcelain: Laguna Frost (WC437) and #16 (WC617), Standard 365 Grolleg and 213, Aardvark Nara 5, Archie Bray Cone 6 Porcelain.
  • Cone 10 stoneware: Laguna B-Mix 10 (WC379), AMACO No. 38 White (best at cone 10), Aardvark KGBS and Vegas Buff.
  • Cone 8 to 10 porcelain: Standard 257 Grolleg, Aardvark Coleman Porcelain and Nara Porcelain.

On Orton's chart for self-supporting cones at 108°F per hour, cone 5 is 2,167°F (1,186°C), cone 6 is 2,232°F (1,222°C) and cone 10 is 2,345°F (1,285°C). Our pottery cone chart has the full table. Under-firing hurts either clay: AMACO lists No. 38 stoneware at 7% absorption at cone 5 against 1.4% at cone 10, so a cone 10 body in a cone 6 kiln stays porous.

Absorption and vitrification: what the data sheets say

Absorption is the share of water a fired test bar soaks up. The lower it is, the more fully the body has vitrified (melted into a tight, partly glassy mass), and the less a mug will weep or a planter will soak up water. Here is what the makers publish for the bodies above.

Clay bodyTypeConeShrinkageAbsorptionFired color (maker)
Laguna B-Mix 5 (WC401)Stoneware512%2.3%Cream in oxidation
AMACO No. 46 BuffStoneware5 (range 5 to 10)12% at 51.8% at 5; 0% at 10Buff at 5, soft gray at 10
AMACO No. 16 White ChocolateStoneware5 to 613.9% at 60.3% at 6Creamy tone; fired color not published
Standard 182 Angel WhiteStoneware6 to 1011.0% at 63.0% at 6; 1.5% at 10Near white
Aardvark Bee Mix 5Stoneware512%2.5%Off-white
Laguna B-Mix 10 (WC379)Stoneware1013%1%Gray-white in reduction
Aardvark KGBSStoneware1012%0%Gray
Laguna Frost (WC437)Porcelain611%0.5%White, translucent
Laguna #16 (WC617)Porcelain6 (title says ^5)13.9%0.12%Very light gray wet
Standard 365 GrollegPorcelain613.5%0.35%White, translucent when thin
Standard 213Porcelain612.0%2.0%White
Aardvark Nara 5Porcelain512%1.1%Gray-white (product page), white (spec sheet)
Archie Bray Cone 6 PorcelainPorcelain611%1%Creamy white in oxidation
Standard 257 GrollegPorcelain8 to 1014.0% at 100.75% at 8; 0.5% at 10White, translucent
Aardvark Coleman PorcelainPorcelain1013.5%0%White

Two things stand out. First, porcelain is usually tighter, but not always: AMACO's White Chocolate stoneware lists 0.3% at cone 6, lower than Standard's 213 Porcelain at 2.0% and Archie Bray's Cone 6 Porcelain at 1%. Second, the cone matters as much as the type: Standard 182 drops from 3.0% at cone 6 to 1.5% at cone 10.

Aardvark's spec sheet gives its shrinkage figures as plus or minus 2% and absorption as plus or minus 1%. Aardvark's spec sheet lists Nara 5 as white, while its cone 5/6 product page calls it gray-white. Laguna's #16 page title says ^5 while its spec field says cone 6. Treat every figure as a guide and test at your own cone and firing schedule.

Shrinkage, warping and drying

Shrinkage overlaps more than most people expect. In the table, stoneware runs 11% to 15% and porcelain 11% to 14%, so a porcelain does not automatically shrink more. Laguna's Frost is one of the lowest bodies listed, at 11%.

Movement is the bigger difference. Because so much of porcelain turns to glass, it softens more at the top of the firing, and wide plates and flared bowls can slump or go oval. Stoneware has more unmelted material holding it up, so it keeps its shape better. Porcelain also cracks at rims and bases more readily if it dries unevenly, so it needs slow, covered drying. Plan for one body's shrinkage when you make lids, sets or anything that must fit.

On the wheel and at the table: how they handle

Stoneware is the easier clay to learn on. It takes water, stands up through several pulls and forgives an uneven hand. Grogged stonewares suit slabs, coils and large pieces because thick walls dry and fire more evenly.

Porcelain feels smooth and slick, and it turns to slurry fast if you use much water. It throws thin and light but tears more easily at soft leather hard, and joins need to be made at the same moisture level. Many potters learn on stoneware first and then move to a plastic porcelain such as Laguna #16. Our porcelain throwing tips page goes step by step.

Color, glazes and translucency

Porcelain's white body makes glazes brighter and clearer. Celadons, clears and pale transparent glazes look the way they do on the maker's white test tile, and underglaze colors stay true. Thin porcelain made for translucency, such as Laguna Frost and Standard 365 or 257, lets light through.

Stoneware gives a warmer base. Buff, speckled and brown bodies show iron flecks and darken through transparent glazes, which many potters prefer for rustic or earthy ware. White stonewares such as Laguna B-Mix 5 or Standard 182 get close to porcelain's brightness while keeping stoneware handling. Glaze fit varies body by body: Laguna lists a COE of 7.14 for Frost and 6.07 for B-Mix 5, so a glaze that fits one may craze or shiver on the other. Use glazes rated for your cone and test each new body; see our cone 6 glazes guide.

Strength, chips and everyday use

Both clays make durable everyday ware when fired to their maturing cone. Dinnerware makers such as Lenox describe porcelain as the more durable of the two, but thin porcelain rims can still chip, and thick stoneware takes knocks well but weighs more. Wall thickness, glaze fit and the right cone matter more than the word on the box.

Both can crack from sudden temperature changes, so neither should go from the fridge straight into a hot oven. If you want ovenware, look for it on the maker's list of uses: Laguna lists ovenware among the applications for B-Mix 5 and B-Mix 10, but not for Frost or #16. Food safety depends on the glaze as well as the clay; a maker's label describes their own test results, not your pots, so fire to the stated cone and test.

Cost and buying

Porcelain usually costs more per pound, but the gap varies by maker. On the makers' own price lists in November 2026, before shipping:

  • Laguna: Frost and #16 porcelain list at about $1.20 to $1.40 per lb, sold in 50 lb steps; both showed as sold out when we checked.
  • Aardvark: cone 5 stonewares list at about $17 to $26 per 25 lb bag, with Nara 5 porcelain just above that range (Nara 5 showed as out of stock).
  • Archie Bray: its Cone 6 Porcelain works out to roughly $0.95 to $1.05 per lb in a 50 lb box.
  • AMACO: No. 16 White Chocolate stoneware sells in 20 lb boxes of 5 lb blocks and works out to about $2 to $2.20 per lb, more than several porcelains.

Freight often costs more than the price gap, so a nearby dealer can matter more than the clay type. Check the live price. Our how much does clay cost guide covers per-pound budgets and why porcelain runs higher.

Can you use both in one studio?

Yes, with a few rules. Fire them together only if both bodies are rated for the same cone. Keep separate reclaim buckets, because a mixed body has untested shrinkage and fit and loses porcelain's whiteness. Clean the wheel and tools when you switch, since stoneware grit shows in porcelain. Join only like with like, as the two bodies shrink differently.

Where does earthenware fit? It is the third main group, fired much lower and left more porous. Our stoneware vs earthenware comparison covers that choice, and types of pottery clay explains all three.

Safety: both clays contain crystalline silica, and porcelain dust is very fine. Laguna's product pages carry a California Prop 65 warning for crystalline silica. Wet clean your studio, never dry sweep, and wear a NIOSH-approved respirator when you mix dry clay or handle dry scraps. Kilns get hot on the outside and need the clearance and ventilation set out in the maker's manual.

Choose stoneware or porcelain

Choose stoneware if

  • You are learning to center and throw, or you hand-build slabs and coils.
  • You want warm, speckled or earthy surfaces, or you make planters and larger forms.
  • You want the most choice at your kiln's cone and a lower price per pound from most makers.
  • You fire a cone 6 kiln and want a body with a long track record, such as Laguna B-Mix 5 or AMACO No. 46.
Popular cone 5 stonewareLaguna B-Mix 5 (WC-401) cone 5 moist clay, 25 lb (5 lb B083Y515RR; 50 lb B083Y4CC1F)
Key specs Cone 5; fires cream in oxidation; 12% shrinkage; 2.3% absorption (Laguna) or 2.75% (Clay-K

Choose porcelain if

  • You want the brightest glaze color, true underglaze color or translucent thin pieces.
  • You already throw well and can work with little water and slow, even drying.
  • You make small to medium pieces, cups, jewelry or tiles rather than wide platters.
  • Your kiln reaches the body's cone, for example cone 6 for Laguna Frost or Standard 365.
Translucent cone 6 porcelainLaguna Frost Porcelain WC437 Cone 6 Moist Clay
Key specs Cone 6; 11% shrinkage; 0.5% absorption; white, translucent

What you need

Whichever you choose, buy a body rated for your kiln's top cone, glazes rated for the same cone, and a 25 lb box to test before you commit. Our best clay for pottery guide compares stoneware and porcelain bodies, and the best kilns for home pottery guide covers cone 6 and cone 10 kilns.

Sources: Laguna Clay product pages for WC401 B-Mix 5, WC379 B-Mix 10, WC437 Frost and WC617 #16 Porcelain (cone, shrinkage, absorption, COE, applications, price, Prop 65 notice); Standard Clay product pages for 182 Angel White, 213 Porcelain, 257 Grolleg Porcelain and 365 Grolleg Porcelain, and its Porcelain and White Stoneware collection; AMACO product pages for No. 46 Buff Stoneware, No. 38 White Stoneware and No. 16 White Chocolate; Aardvark Clay clay specifications sheet and cone 5/6 clay listing; Archie Bray Clay Cone 6 Porcelain product page; Orton pyrometric cone chart (self-supporting cones, 108°F per hour); Lenox and Made In dinnerware guides; Wikipedia entry on bone china. Specs checked November 2026.

Frequently asked questions

What is better, ceramic or stoneware plates?

Stoneware is a type of ceramic, so the real question is which ceramic. Plates sold simply as "ceramic" are often lower-fired earthenware, which is more porous and chips more easily, while stoneware and porcelain are fired hotter and come out denser. For everyday plates, a well-fired stoneware or porcelain is usually the harder-wearing choice; our stoneware vs earthenware page compares the lower-fired option.

What is bone china made of?

Bone china is a porcelain made with bone ash. The traditional recipe is roughly half bone ash with the rest kaolin and china stone, and a British industry definition calls for at least 30% phosphate from calcined bone or calcium phosphate. It is a factory product: US clay makers do not sell it as a moist clay body for home kilns.

Is porcelain considered high end?

Porcelain is often marketed as the formal, special-occasion choice, and fine thin porcelain and bone china sit at the top of many dinnerware ranges. But porcelain is also used for everyday restaurant ware, so the material alone does not make a piece high end. For a home potter, porcelain clay costs a little more per pound than most stoneware and takes more skill to throw.

Can you fire stoneware and porcelain in the same kiln load?

Yes, if both bodies and their glazes are rated for the same cone. A cone 6 stoneware and a cone 6 porcelain can share a load; a cone 10 porcelain in a cone 6 firing will stay porous. Set wide porcelain forms on a flat, clean shelf, as they move more at the top of the firing.

Do stoneware and porcelain need different glazes?

Not by type, but by cone and fit. Use glazes rated for the cone you fire, and test each new body, because the clays expand and shrink by different amounts. Laguna lists a COE of 7.14 for Frost porcelain and 6.07 for B-Mix 5 stoneware, so the same glaze can fit one and craze on the other.

Can you join porcelain to stoneware?

It is risky. The two bodies usually shrink by different amounts and at different rates, so a porcelain handle or sprig on a stoneware pot can crack at the join in drying or firing. Join like with like, or test the pairing on small pieces first.

Researched and written by Muhammad Mustafa

Muhammad Mustafa researches and writes Home Pottery HQ from maker spec sheets, manuals, dealer listings and published studio guidance. He does not claim hands-on testing of products he has not used, and every page names its sources.

Specifications and availability change often. Check the product listing before you buy, and follow the manufacturer's manual for setup, weight limits and maintenance. We do not print prices because they change daily; the buttons take you to the live price. Read our affiliate disclosure.