Verdict
Mayco Stroke and Coat is the most flexible glaze a home potter can buy. You can paint it like an underglaze, it fires to a gloss with no clear coat, and Mayco rates it from cone 06 to 10 in oxidation or reduction. That means one set of jars works in a low-fire class kiln and a cone 6 home kiln. The Kit #1 sampler of 12 colors is the easiest way in.
The trade-offs: it is a glaze, so thick coats can move; some light colors fade at cone 5/6; and Mayco's own documents disagree slightly on the top of the cone range. This review is research-based, built from Mayco product pages, kit pages and its 2023 brochure, checked October 2026. We did not fire the colors ourselves.
Spec table
| Spec | Mayco Stroke & Coat |
|---|---|
| Product type | Glaze (Mayco: "the industry's most versatile glaze") |
| Surfaces | Wet clay, earthenware bisque, stoneware bisque |
| Cone range | 06 to 10, oxidation or reduction (product pages) |
| Coats | 1 coat translucent; 2 to 3 coats full opacity |
| Finish | Gloss without clear glaze |
| Sizes | 2 oz and 8 oz squeeze bottles, pint, gallon |
| Labels (SC-15, SC-74) | ACMI AP seal; dinnerware safe |
| Mixing | Colors are intermixable; thin with water or media for washes |
Source conflict: Mayco's Stroke & Coat product pages (for example SC-15 Tuxedo) say cone 06 to cone 10. Mayco's 2023 Stroke & Coat brochure says the line "can be fired from cones 06 to 6, with most colors reaching cone 10." If you fire at cone 10, check each color's cone 10 chip before relying on it.
Is Stroke and Coat a glaze or an underglaze?
Mayco is clear that Stroke and Coat is a glaze. It contains enough glass formers and fluxes to melt into a glossy surface by itself, which an underglaze does not. It gets confused with underglaze because it is thick, heavily pigmented and brushes on with crisp edges, so many people use it for painted designs the way they would use an underglaze. School Specialty, for example, lists it as Stroke & Coat Wonderglaze, which is why "wonder glaze" turns up in searches.
Because it is a glaze, a clear coat is optional rather than required. The brochure says you can add a clear such as NT-CLR Clear One Dipping Glaze or S-2101 Crystal Clear Brushing if you want. For a full side-by-side with the best-known underglaze, see Velvet vs Stroke and Coat.
Stroke and Coat colors and kits
Stroke and Coat colors carry SC numbers, from SC-1 Pink-A-Boo up past SC-100 on Mayco's site, plus a separate Speckled Stroke & Coat range with added specks. Mayco sells three 12-color kits in 2 oz bottles and in pints. The two most popular are below.
Stroke & Coat Kit #1 (SC-KIT1)
Kit #1 is picked because it covers a full basic palette, including a white and a black, which makes it easy to mix tints and shades. Mayco lists 12 colors: SC-16 Cotton Tail, SC-6 Sunkissed, SC-75 Orange-A-Peel, SC-74 Hot Tamale, SC-18 Rosey Posey, SC-13 Grapel, SC-11 Blue Yonder, SC-12 Moody Blue, SC-26 Green Thumb, SC-36 Irish Luck, SC-14 Java Bean and SC-15 Tuxedo.
- Contents: 12 x 2 oz squeeze bottles
- Cone: 06 to 10 (product pages)
- Coats: 2 to 3 for opacity
- Also sold as: SC-KT1P pints kit
Pros
- Primary palette plus black and white
- Small bottles for testing
- One kit works low and mid fire
Cons
- 2 oz goes fast on large pieces
- Reds and yellows may shift at cone 6
Who should skip it: potters who want pastels; Kit #2 has more pinks and soft blues.
Stroke & Coat Kit #2 (SC-KIT2)
Kit #2 is picked as a companion palette with fewer primaries and more pinks, teals and browns. Mayco lists SC-16 Cotton Tail, SC-24 Dandelion, SC-1 Pink-A-Boo, SC-17 Cheeky Pinky, SC-3 Wine About It, SC-30 Blue Dawn, SC-28 Blue Isle, SC-10 Teal Next Time, SC-8 Just Froggy, SC-20 Cashew Later, SC-25 Crackerjack Brown and SC-15 Tuxedo.
- Contents: 12 x 2 oz squeeze bottles
- Overlap with Kit #1: Cotton Tail (white) and Tuxedo (black)
- Also sold as: SC-KT2P pints kit
Pros
- Softer colors
- Good add-on to Kit #1
Cons
- Pinks and light tans are the shades Mayco says can fade at cone 5/6
Who should skip it: cone 6 potters who want strong, stable color; test the pinks first.
Speckled Stroke & Coat (SP series)
Speckled Stroke & Coat is the same heavily pigmented, brushable glaze with small specks of a contrasting color added. Mayco describes the line as "Stroke & Coat colors with small specks of contrasting hues to add dimension and visual appeal." The codes start with SP instead of SC, and many are speckled versions of familiar colors, such as SP-274 Speckled Hot Tamale, SP-211 Speckled Blue Yonder and SP-210 Speckled Teal Next Time. Mayco's line page shows about 30 colors.
It works like regular Stroke & Coat: one coat is translucent, two to three coats give full opacity, and it fires glossy without a clear. Mayco's line page says the range matures at cone 06/05 and that cone 6 behavior is noted color by color, while the SP-274 product page lists cone 06 to 10. At cone 6, Mayco says SP-274 lightens to a medium brown and the specks remain. Sizes for SP-274 are 2 oz and 8 oz squeeze bottles and pints, and it carries the AP seal and a dinnerware safe icon.
Speckles are a quick way to get a stoneware-style look on low-fire earthenware or ready-made bisque. As with any color, check the cone 6 note before firing higher, since the base color can shift even when the specks hold.
Stroke and Coat color chart: how to read it
The Stroke and Coat color chart on Mayco's site shows fired chips at three settings: cone 06 on white earthenware, cone 6 in oxidation on white stoneware, and cone 10 in reduction on white stoneware. Under some chips Mayco adds a short note. SC-15 Tuxedo, for example, is "Opaque. No color change" at cone 6. SC-74 Hot Tamale is "Semi-Transparent. No color change" at cone 6.
Mayco's 2023 brochure gives a general rule for the whole range: darker hues such as red, orange, yellow, blue and green may darken at cone 5/6 and up, while lighter shades such as tan, purple and pink will fade. Use the chip that matches your cone and clay color, and paint a test tile with one, two and three coats so you can see the change for yourself.
Print the chart only as a rough guide. Screens and printers shift color. A row of fired test tiles on your own clay is the only chart you can trust.
How to use Mayco Stroke and Coat
- Shake the bottle well; the glaze is thick and pigment settles.
- Wipe bisque with a damp sponge to remove dust. On greenware, work on wet or leather-hard clay.
- Brush the first coat evenly. It will look streaky and translucent.
- Let it dry until the shine is gone, then add a second and third coat for solid color.
- Keep the foot and the bottom edge clean, or wax them first.
- Fire to the cone you planned. Mayco's brochure says Stroke & Coat on wet or leather-hard clay can be fired to cone 04 in a single firing.
Our full guide on how to glaze pottery covers thickness, wax resist and faults in more detail.
Stroke and Coat glazes in practice: popular uses
Solid color on bisque
The most common use is plain, even color on a bisque mug, bowl or tile. Three coats of one color gives a flat, glossy result that looks much like the cone 06 chip. Mayco's brushing advice for its Elements line is to let the wet shine disappear before the next coat, and the same habit helps here: wet-on-wet coats drag and leave thin streaks.
Painted designs and washes
Because the glaze is thick and holds an edge, it works for lettering, florals and pattern work. Mayco says the colors can be thinned with water or media for wash effects, so one bottle covers both a solid band and a soft, watercolor-like shade. A single coat stays translucent, which is useful for shading over a lighter base color.
Mixing your own colors
Mayco lists Stroke & Coat colors as intermixable. Adding SC-16 Cotton Tail lightens a color into a pastel, and a little SC-15 Tuxedo deepens it. Mix enough for the whole project at once and note the ratio, since matching a mix later is hard.
Over or under other glazes
Stroke & Coat is often combined with Mayco's other lines, and Mayco's glaze combination page shows layered results at each cone. Any layering adds thickness, so test combinations on a tile before using them on the lower third of a tall piece. Our clay and glazes hub explains why thick, flowing layers run.
Sizes: which bottle to buy
The 2 oz squeeze bottle suits testing, detail and small pieces. The 8 oz bottle is a middle step for colors you use often. Pints and gallons make sense for a studio or a class, or for a single color you plan to use as a main glaze on many pots. If you are starting from nothing, a 12-color 2 oz kit and a pint of your favorite base color is a sensible first order.
What it does well
- One jar, many kilns: rated cone 06 to 10 on the product pages, in oxidation or reduction.
- No clear needed: fires glossy on its own, which saves a step and a jar.
- Painterly control: thick enough for crisp brush strokes; thin with water for washes.
- Intermixable: colors blend into new shades.
- Dinnerware labels: the colors we checked (SC-15, SC-74) carry the ACMI AP seal and a dinnerware safe icon.
Weak points
- Color shifts at mid fire: light colors fade and dark ones deepen at cone 5/6 per Mayco.
- It can move: it is a true glaze, so very heavy coats near the foot can run.
- Cone 10 wording differs between product pages and the brochure.
- Small bottles: 2 oz is enough for testing and small pieces, not for covering many large pots.
Food safety
Mayco's brochure describes Stroke & Coat as "AP Certified Non-Toxic, Food Safe and Dinnerware Safe when used according to manufacturer's directions," and the product pages we checked carry a dinnerware safe icon. That is the maker's label, not a promise about your pot. Results depend on firing to the stated cone, a compatible clay and a sound, uncrazed surface. Mayco also says food-contact ware is best on mid-range or high-fire clay (cone 5 to 10).
Who should buy it
- Beginners who want bright, predictable color without learning dipping.
- Home potters who share a kiln that fires both low and mid range.
- Anyone painting designs who wants a glossy finish in one step.
Who should skip it
- Potters who want flowing, reactive surfaces; look at Mayco Stoneware glazes instead.
- Anyone glazing many large pieces, where a dipping bucket is cheaper per pot.
Alternatives
If you want a true underglaze under clear, AMACO Velvet is the usual comparison; see our Velvet review and the best underglazes guide. For the rest of Mayco's catalog, read our Mayco glazes review. For cones and labels across brands, the clay and glazes hub has the background.
Sources: Mayco Stroke & Coat line page; Mayco product pages SC-15 Tuxedo and SC-74 Hot Tamale; Mayco SC-KIT1 and SC-KIT2 kit pages; Mayco product kits index; Mayco 2023 Stroke & Coat brochure (dealer-hosted PDF); Mayco Dinnerware Suitability and ACMI page; School Specialty listing name "Stroke & Coat Wonderglaze"; Mayco Speckled Stroke & Coat line page and SP-274 Speckled Hot Tamale product page; Mayco distributors page. Specs checked October 2026.