What wax resist does
Wax resist is the simplest way to keep glaze where you want it. Mayco describes its AC-302 as a water-based coating that repels glaze, which dissipates in the kiln and leaves the surface as it was before firing. AMACO calls its product a wax emulsion that resists glaze, slip and underglaze on greenware or bisque.
Potters use it for two jobs. The everyday job is waxing the foot and any surface that touches the kiln shelf or a lid, so glaze cannot fuse the pot to the shelf. The creative job is painting lines, dots and shapes in wax so a glaze or underglaze breaks around them, a technique Mayco calls batik when wax is layered between coats of color.
This guide is research-based: it draws on the makers' product pages and instructions, US dealer listings and published potter articles. We do not test products ourselves. Our how to glaze pottery guide covers where waxing fits in the full glazing order.
Wax resist products compared
All four products below are cold, water-based wax emulsions you brush straight from the jar. They differ in tint, sizes and advice on waxing over glaze.
| Product | Tint | Sizes | Use on (per maker or dealer) | Key note | Price |
|---|---|---|---|---|---|
| Mayco AC-302 Wax Resist | Not tinted | 2 oz squeeze bottle, pint, gallon | Greenware, bisque, over unfired color | One heavy coat; second coat will not adhere | Check price |
| AMACO Wax Resist | Not tinted | Pint, gallon | Greenware or bisque; resists glaze, slip, underglaze | May peel dipping glazes or glazes without gum | Check price |
| Aftosa Green Wax Resist | Green, fires clear | 4 oz, quart (dealers) | Bases, rims, brushed or trailed designs | Needs red heat to burn off | Check price |
| Aftosa Black Wax Resist | Black, leaves a fired line | 4 oz, pint (dealers) | Decorative lines, cone 06 to 8 | Line fades at higher cones | Check price |
Price bands at US dealers in November 2026: Mayco AC-302 about $4 to $6 for 2 oz and $12 to $15 a pint; AMACO about $20 to $30 a pint and $100 to $120 a gallon; Aftosa Green about $4 to $5 for 4 oz and $30 to $40 a quart; Aftosa Black about $8 to $10 for 4 oz and $28 to $32 a pint. Check the live price.
Mayco AC-302 Wax Resist
Mayco says AC-302 can go on unglazed greenware or bisque, or over previously applied, unfired color. Its instructions ask for one heavy coat, because even a thin coat repels color and a second coat will not stick to the first. Once on, it can only be removed by firing. The 2 oz squeeze bottle is the easy size for waxing a few feet at home.
Who should skip it: Studios that wax dozens of pots a week, who save with a gallon of any brand.
AMACO Wax Resist
AMACO's wax emulsion resists glaze, slip and underglaze on greenware or bisque, and AMACO labels it non toxic. AMACO also gives the clearest warning in this category: used over dipping glazes, or over glazes without gum added, its wax may peel the glaze off the ware. AMACO points to its Gum Solution for reviving old glazes. It comes in pints and gallons, with no small bottle.
Who should skip it: Potters who mostly wax over unfired dipping glaze, unless they test first.
Aftosa Green Wax Resist
Aftosa tints this wax green so you can see where it went, and it fires clear. We could not find an Aftosa maker page, so these details come from The Ceramic Shop and Sheffield Pottery listings. They say to brush it or trail it for designs, thin it to suit, let it dry 3 to 4 hours before glazing or a second coat, and fire to at least cone 017, red heat, for it to burn off.
Who should skip it: Anyone in a cold climate ordering in winter; dealers warn frozen wax turns lumpy and stops resisting.
Aftosa Black Wax Resist
Aftosa's black wax resists glaze like the others but leaves a black oxide line when fired, per The Ceramic Shop. The listing gives a working range of cone 06 to cone 8, says the black fades at higher temperatures and is gone around cone 10, and suggests a clear overglaze to darken a gray line. Because it leaves colorant behind, read the SDS and treat it as decoration.
Who should skip it: Cone 10 potters, and anyone who only wants to keep glaze off feet.
Latex and hot wax: the other resists
Latex resist dries to a rubbery film that you peel off before firing, so you can glaze over a design, lift the latex and glaze the bare area in a second color. Big Ceramic Store's tips say to apply one thick coat, lift it with a needle tool and wear a dust mask while peeling, since dry glaze comes off with it. Hot paraffin dipping gives a clean, level foot line, but it is a fire risk: keep the heat low, stop if it smokes and keep an extinguisher close. For a home studio, a cold emulsion is the safer default.
How to apply wax resist
- Start with clean, dust-free bisque or greenware. Wipe bisque with a barely damp sponge if it is dusty, and let it dry.
- Pour a small amount of wax into a cup. Aftosa's dealers say never to pour used wax back into the jar, because glaze and clay contaminate it.
- Coat your brush in liquid dish soap and wipe off the excess. Mayco's own lava lamp tile project does this with a liner brush, and Aftosa's dealers recommend it too.
- Brush one even, heavy coat where glaze must not go. For a foot, cover the bottom and the lowest part of the foot ring; for a lidded jar, the gallery and the lid flange.
- Let the wax dry fully before glazing. Aftosa's listings give 2 hours minimum on one page and 3 to 4 hours on others; Mayco gives no time, only "dry."
- Dip, pour or brush your glaze. It will bead up on the wax.
- Wipe or pounce the beads off the wax with a clean, damp sponge. Mayco warns that any color left on the wax will stick to the fired surface.
- Load with a little extra space around waxed pieces, and fire to the glaze's cone.
Keep a cheap brush just for wax and mark its handle. Wax traces in a glaze brush will spoil your next glaze job.
Decorative wax resist: lines, patterns and layered glaze
For patterns, paint wax with a liner or round brush, or load it into a slip trailer for raised lines and dots (see slip trailing for the tool). Wax bare bisque, glaze over it, and the clay shows through. For a layered look, brush a first glaze, let it dry, wax a design over it, then apply a second glaze. Mayco's lava lamp tile works this way: wax circles over dried layers of SC-77 Glo-Worm and SC-27 Sour Apple, then three coats of SC-76 Cara-bein Blue over the whole tile, fired to cone 06.
Before waxing over unfired glaze, read the label. Mayco says AC-302 can go over unfired color, while AMACO warns its wax may lift dipping glazes and glazes without gum. Test on a tile first. Mayco also says its wax tends to chip if you try to scratch through it, so it is a poor partner for sgraffito lines.
Wax resist with underglaze and slip
Wax works the same way over greenware or bisque before underglaze or slip: paint the wax, brush the color over it, and the waxed areas stay clean. Our underglaze techniques guide shows where wax fits among other methods, and mishima covers inlaid lines, which some potters combine with wax.
Drying, firing and burn off
Wax does its work during glazing only. Once the glaze is on, the wax has nothing more to do, and it burns away early in the firing. Aftosa's dealers say the kiln has to reach red heat, at least cone 017, for the wax to burn off; wax on raw greenware burns away in the bisque firing.
Burning wax smokes. Mayco tells potters to give the kiln extra ventilation early in the firing to clear those fumes, and to leave extra room when loading because repelled color can flake off and land on nearby pieces. A kiln vent or an open, well ventilated room helps; see our kiln vent guide. Mayco also notes wax only repels glaze while you apply it: a heavy, runny glaze can still flow over a waxed foot in the kiln, so leave a bare margin for glazes that move.
Cleanup: brushes, spills and mistakes
Clean brushes straight after use. Aftosa's dealers recommend warm, soapy water. Mayco says its wax needs no brush preconditioning, and if it dries in a brush, mineral spirits will remove it. (A dealer listing that reproduces Mayco's label text suggests conditioning the brush with Mayco's AC-525 Brush Cleaner, so the two Mayco sources differ; soap works either way.)
Wax in the wrong place is harder. Mayco says a coat can only be removed by firing. The fix is to fire the piece again as bisque, which Aftosa's dealers describe as re-firing at cone 06, then re-wax and glaze. Ceramic Arts Network's wax pattern article gives the same advice for a flawed waxing. Sponge glaze beads off waxed areas with a damp sponge rather than scraping them dry.
Storage and shelf life
Keep the lid tight. Dealers say Aftosa wax lasts 2 to 3 years, that a strong sour smell means it is contaminated, and that wax which freezes turns lumpy and will not resist properly. Store any wax indoors, away from frost.
Common wax resist mistakes
- Glazing over wet wax. The glaze sticks where the wax has not set. Wait until it is dry.
- Adding a second coat of Mayco wax. Mayco says it beads up and will not adhere to the first.
- Leaving beads on the wax. Any glaze left on a waxed foot fires onto it and can stick to the shelf.
- Waxing over dipping glaze without a test. AMACO warns the wax may peel the glaze off.
- Returning wax to the jar. Pour out what you need and discard leftovers.
- Waxing right to the edge of a runny glaze. Leave a wider bare band above the foot for glazes that move.
- Firing a full load of waxed pots with no ventilation. Expect smoke early in the firing.
Safety notes
Wax resist itself is low risk, but the glaze you wipe off it is not. Glaze and clay dust contain silica, so wipe beads with a damp sponge, clean up wet and never sand or dry brush glaze off waxed areas. Wear a NIOSH-approved respirator when mixing dry glaze materials, and read the maker's SDS for each wax and glaze; see our clay dust safety guide. Hot paraffin is a fire risk and should not be heated on a kitchen stove you cook on.
Wax keeps glaze off the foot; it does not change whether a glaze is food safe. Follow each glaze's label, fire to the stated cone and test your own results before using a piece for food.
What you need
A bottle of water-based wax resist, a cheap brush kept for wax, a small cup, a damp sponge and dish soap cover most home glazing. For which brushes to buy and which to keep for wax, see our pottery brushes guide.
Sources: Mayco AC-302 Wax Resist product page and Mayco Wax Resist color page (application and helpful hints); Mayco projects Lava Lamp Technique Tile and Canvas Pouring with Wax Resist; AMACO Wax Resist product page; dealer listings for Aftosa Green and Black Wax Resist at The Ceramic Shop, Sheffield Pottery and Good Earth Clays; Creative Crafts Mayco AC-302 listing; The Ceramic Shop wax resist category; Big Ceramic Store resist tips (two pages); Ceramic Arts Network, "Wax Resist Patterns." Specs checked November 2026.