Verdict
AMACO River Rock is the easiest brown in this group to like: a glossy, opaque glaze that changes from sandy brown to near black and turns amber wherever it crosses texture. It is also one of AMACO's most charted bases, with a whole layering chart of 25 glazes brushed over it. If you want one jar from this page, start there.
The other eight split into jobs. Satin Oribe and Cosmic Tea Dust are steady layering bases. Textured Turquoise, Black Aventurine and June Bug bring movement and sparkle. Ancient Copper has a cooling rule you must follow. Storm and Rainforest are transparent Celadons that pool color in carving.
This guide is research-based: we compared AMACO's shop pages, Potter's Choice sheet, layering chart and combination posts with US dealer listings. We have not fired these glazes; descriptions of results are AMACO's.
The nine glazes at a glance
| Code | Glaze | Line | Finish (AMACO) | Coats | Food label | Light vs dark clay (AMACO) |
|---|---|---|---|---|---|---|
| PC-67 | River Rock | Potter's Choice | Glossy, opaque | Heavy; 2 per layer in AMACO's chart | Food safe (PC sheet) | Not published; chart tiles on No. 46 Buff |
| PC-15 | Satin Oribe | Potter's Choice | Satin, opaque, "burnished" | 2 per layer in AMACO's combos | Food safe (PC sheet) | Not published |
| PC-25 | Textured Turquoise | Potter's Choice | Gloss, fluid | 1 to 3 shown on AMACO's sheet | Food safe (PC sheet) | Over Blue Rutile: best on light clay, "lovely" on dark |
| PC-56 | Ancient Copper | Potter's Choice | Satin at cone 5, glossier at cone 6 | Three thick coats (dealer text) | Food safe (PC sheet) | Not published |
| PC-63 | Cosmic Tea Dust | Potter's Choice | Sparkly, opaque | Heavy (PC sheet) | Food safe (PC sheet) | Not published |
| PC-10 | June Bug | Potter's Choice | Glossy, opaque, crystals | Heavy (PC sheet) | Food safe (PC sheet) | Not published |
| PC-65 | Black Aventurine | Potter's Choice | Fluid black, metallic sparkle | Heavy (PC sheet) | Food safe (PC sheet) | Not published |
| C-27 | Storm | Celadon | Gloss, semitransparent | 3 (Celadon line) | Food safe per dealers | Clay color shows through |
| C-49 | Rainforest | Celadon | Gloss, semitransparent | 3 (Celadon line) | Food safe per dealers | Clay color shows through |
All nine are cone 5 to 6 glazes for cone 04 bisque. AMACO's Potter's Choice sheet says most colors "benefit from a heavy-handed application", but the shop pages for these seven print no coat count. Line-wide details are in our Potter's Choice review.
Food labels: AMACO's Potter's Choice FAQ says every Potter's Choice glaze is food safe except PC-4 Palladium, PC-9 Vintage Gold and PC-64 Aventurine. When we checked in November 2026, the shop pages for River Rock, Satin Oribe and Textured Turquoise showed a Food Safe icon, while the pages for Ancient Copper, Cosmic Tea Dust, June Bug and Black Aventurine did not. Dealer listings call Ancient Copper food safe. Read the label on your own jar before using any of them inside a mug.
Price band: Potter's Choice pints typically $23 to $26 at AMACO's shop in November 2026, June Bug about $35 to $40, Celadon pints about $20 to $25. Check the live price.
PC-67 River Rock
AMACO describes River Rock as sandy, dark brown tones that fade into ebony, turning "rich amber when applied over texture." On vertical surfaces, subtle green-gray honeycomb shapes appear under the amber breaks. It is glossy and opaque, sold in pints and gallons.
- Finish: glossy, opaque
- Coats: two as a base in AMACO's chart; three thick coats alone, per dealer listings
- Sizes: pint, gallon
On light and dark clay: AMACO publishes no dark clay tile; its chart was fired to cone 6 on No. 46 Buff Stoneware. Dealer text says a thin coat looks splotchy, so brush it generously.
AMACO's River Rock combinations: AMACO's chart brushes 25 Potter's Choice glazes over River Rock, two coats each, including PC-15 Satin Oribe, PC-31 Oatmeal, PC-42 Seaweed and PC-53 Ancient Jasper. Its layering library adds River Rock over PCF-75 Moss Mist and over PCF-74 River Birch, and PC-02 Saturation Gold over River Rock.
Pros
- One of AMACO's most charted bases
- Texture turns amber
- Pint and gallon sizes
Cons
- Needs a heavy coat or it looks patchy
- Coat count not printed on AMACO's own page
Who should skip it: anyone after a flat, even brown with no breaking.
PC-15 Satin Oribe
AMACO calls Satin Oribe "a modern take on a traditional Japanese oribe glaze" with "a wonderful blue-green burnished look." Over texture it shows dark green pools and light gray breaks. It is opaque and satin rather than glossy, which is why AMACO so often puts it underneath runnier glazes.
- Finish: satin, opaque
- Coats: two coats as a base in AMACO's published combinations
- Sizes: pint, gallon; AMACO also mentions a dry dipping mix
Satin Oribe glaze combinations from AMACO
AMACO's "Ancient Oribe" is two coats of PC-53 Ancient Jasper over two coats of Satin Oribe at cone 6, which AMACO says gives "an almost metallic luster." Its customer favorites post puts PCF-74 River Birch over Satin Oribe as a stiff base; our River Birch review covers that pairing. The library also lists Satin Oribe over PC-17 Honey Flux, C-10 Snow and PC-10 June Bug, and PC-26 Blue Lagoon over Satin Oribe.
On light and dark clay: not published by AMACO; fire a tile on a dark body.
Pros
- Stable base under fluid glazes
- Satin surface
- Many published pairings
Cons
- Less movement on its own than the glossy greens
- Dry mix behaves differently from the pint
Who should skip it: potters who want a glossy, runny green on its own; look at Seaweed or June Bug instead.
PC-25 Textured Turquoise
AMACO's description is "a subtle turquoise gloss, green-beige where thin, but a beautiful aqua where thick." The shop page calls it fluid. AMACO's sheet shows it at one, two and three coats at cone 5, so thickness controls the color.
- Finish: gloss, fluid
- Coats: one to three shown by AMACO; two over two in its combinations
- Sizes: pint, gallon
On light and dark clay: the one AMACO note comes from its Blue Rutile pairing: two coats of Textured Turquoise over two coats of PC-20 Blue Rutile is "somewhat translucent," shows best on lighter clays but is "lovely on dark clays, too," and should go to cone 5 or 6, "but not hotter." That pairing is covered in our Blue Rutile review.
AMACO's other combinations: "Green Milk Glass" is two coats over two coats of PC-19 Moon River at cone 6. "Electric Storm" is PC-14 Lapis Flow over Textured Turquoise, and AMACO warns "She's a runner!" The library adds Textured Turquoise over PC-10 June Bug and PC-44 Sage, and PC-34 Light Sepia, C-49 Rainforest and PC-42 Seaweed over it.
Pros
- Color shifts with thickness
- Works on texture
- Widely layered
Cons
- Fluid, and more so under other fluid glazes
- Turns green-beige if brushed thin
Who should skip it: anyone glazing to the foot without a catch tray, or anyone who wants one flat turquoise.
PC-56 Ancient Copper
AMACO says Ancient Copper takes its cue from classic tomato red reduction glazes. It is "an iridescent, iron red glaze that breaks dark brown over texture" and pools dark yellow-green for a weathered look. It fires satin at cone 5 and glossier with metallic floats at cone 6. The shop lists it in pints only.
- Finish: satin at cone 5, gloss with metallic floats at cone 6
- Coats: three thick coats, leaving room at the foot (dealer listing of AMACO's text); thin coats look splotchy
Do not slow cool Ancient Copper. AMACO's shop page says to avoid slow cooling, and its combination post says a slow cool turns it brown. Use a fast or natural cool.
Ancient copper glaze combinations from AMACO
AMACO's best-known pairing puts PC-17 Honey Flux next to Ancient Copper with a small overlap, and our Honey Flux combinations guide covers it. AMACO's layering library also lists Ancient Copper over PC-63 Cosmic Tea Dust, PC-53 Ancient Jasper, C-25 Downpour, SH-12 Chai Matte and SH-42 Oolong Matte, and PC-34 Light Sepia or PC-27 Tourmaline over it. The shop page shows it over PC-31 Oatmeal and PCF-54 Flux Blossom.
On light and dark clay: not published by AMACO.
Pros
- Two looks from one jar by cone
- Iron red modeled on reduction glazes
- Many pairings
Cons
- No slow cool
- Pint only
- Patchy if thin
Who should skip it: potters whose kiln program always slow cools, or who fire mixed loads with crystal glazes that need it.
PC-63 Cosmic Tea Dust
AMACO's words: "a sparkly, dark brown glaze, which breaks a light yellow-brown over texture." The sparkle "shifts subtly from silver to copper," giving an iridescent quality. It is opaque and sold in pints and gallons. AMACO's 2019 field guide marked it as not for spraying, so brush it.
- Finish: opaque, sparkling
- Coats: not printed on the shop page; AMACO's sheet advises a heavy application
- Sizes: pint, gallon
AMACO's Cosmic Tea Dust combinations: it works both ways. On top, AMACO's library shows it over PCF-74 River Birch, PCF-75 Moss Mist, PC-38 Iron Yellow, C-27 Storm and SH-46 Matcha Matte. As a base, it sits under PC-40 True Celadon, PC-44 Sage, PC-61 Textured Amber and PC-56 Ancient Copper.
On light and dark clay: not published by AMACO.
Pros
- Sparkle without a special firing
- Strong base for greens
- Pint and gallon
Cons
- Not for spraying per AMACO's field guide
- Dark color hides fine carving
Who should skip it: anyone wanting a light, warm brown; River Rock or Oatmeal is closer.
PC-10 June Bug
June Bug is a "glossy, dark green metallic glaze that develops small triangular iridescent crystals," per AMACO. It is opaque and, unlike most glazes here, holds its color over texture rather than breaking. AMACO shows test cups at cone 5 and cone 6. It is sold in pints.
- Finish: glossy, opaque, iridescent crystals
- Coats: not printed on the shop page; heavy application per AMACO's sheet
- Sizes: pint
AMACO's June Bug combinations: June Bug is mostly a base in AMACO's library, under PC-30 Temmoku, PC-15 Satin Oribe, PC-25 Textured Turquoise, PC-59 Deep Firebrick and PC-64 Aventurine. AMACO also shows June Bug over PC-16 Purple Crystal. For more on the Temmoku side, see our temmoku glaze guide.
On light and dark clay: not published by AMACO.
Pros
- Metallic crystal surface from the jar
- Stays even over texture
- Good base
Cons
- Pint only
- Higher price band than most Potter's Choice
Who should skip it: anyone who wants texture to break light; June Bug covers it instead.
PC-65 Black Aventurine
AMACO describes Black Aventurine as "a fluid, rich black glaze that develops a metallic sparkle," and adds that a slow cool grows crystals. It is a different glaze from PC-64 Aventurine, which AMACO's FAQ lists as not food safe. Pints only.
- Finish: fluid, opaque black with sparkle; crystals if slow cooled
- Coats: not printed on the shop page; heavy application per AMACO's sheet
- Label note: AMACO's page carries a California Prop 65 warning for lithium carbonate
AMACO's Black Aventurine combinations: the library lists it over PCF-3 Midnight Run and over PC-16 Purple Crystal, and AMACO's database pairs it over PC-19 Moon River.
On light and dark clay: not published by AMACO.
Pros
- Deep black with sparkle
- Crystals as an option with a slow cool
Cons
- Fluid
- Few published pairings
- Prop 65 lithium warning means extra care in handling
Who should skip it: potters who fire Ancient Copper in the same load, since one wants a slow cool and the other must not have one.
The two Celadons: Storm and Rainforest
Storm and Rainforest are not Potter's Choice glazes. AMACO files both under its Celadon line: transparent, "100% mixable" glosses that pool color in carving. Line-level details such as mixing ratios and clay choice belong to our AMACO Celadon review, so these two get short sections here.
C-27 Storm
AMACO calls Storm "a deep, glossy navy that pools and accents textured ware." It is semitransparent and sold in pints, gallons and a 10 lb dry mix. Do not confuse it with DL-27 Storm Cloud, a Dipping and Layering glaze. AMACO's library shows C-10 Snow over Storm, Storm over C-10 Snow, Storm over SH-21 Acai Gloss and PC-63 Cosmic Tea Dust over Storm.
Pros
- Rich navy in carving
- Mixable with other Celadons
- Dry mix for dipping
Cons
- A blue, not an earth tone
- Transparent, so clay color changes it
Who should skip it: anyone wanting an opaque navy over a dark body.
C-49 Rainforest
Rainforest is "a deep, glossy forest green that pools and accents textured ware," per AMACO, sold in pints and a 10 lb dry mix. The library lists it over PC-25 Textured Turquoise, PC-26 Blue Lagoon and PC-31 Oatmeal, and C-10 Snow over Rainforest.
Pros
- Classic green celadon depth
- Mixable
- Dry mix available
Cons
- No gallon listed
- Transparent, so it needs texture to look its best
Who should skip it: potters with smooth, untextured forms who want strong color.
How to apply this group
- Bisque to cone 04, then wipe the piece with a damp sponge.
- Brush Potter's Choice colors on heavily, letting each coat dry. For layering, follow AMACO's charts: two coats of the base, then two coats of the top glaze.
- Brush the Celadons in three coats, pushing glaze into texture.
- Stop fluid glazes (Textured Turquoise, Black Aventurine and stacked combinations) well above the foot, and use a catch tray.
- Fire to cone 5 or 6 with a witness cone. Use a natural or fast cool for Ancient Copper; save slow cools for loads without it.
AMACO prints two sets of cone temperatures. Its line pages give cone 6 as 2,232°F (1,222°C), while product sheet text repeated by dealers gives 2,266°F (1,241°C) with the last 200°F (100°C) climbing at 270°F (150°C) per hour. Fire by cone, not by a number. Our AMACO glaze layering guide covers stacking order and thickness.
Food surfaces and labels
AMACO's food label describes one glaze fired correctly on its own. A layered combination is a new glaze that no one has tested on your clay. Fire to the stated cone, keep fluid stacks off the inside of mugs and bowls until tested, and see our food safe glaze guide for what testing involves.
Who should buy this group, and who should skip it
Buy these glazes if you fire at cone 5 to 6, like browns and greens that break over texture, and want maker-published combinations to copy. River Rock, Satin Oribe and Cosmic Tea Dust make a sensible first set of bases.
Skip them if you fire low fire only, want flat even color, or cannot control cooling (Ancient Copper and Black Aventurine both depend on it).
Alternatives and related AMACO earth tones
For Mayco's brown and wood-tone glazes, see our Mayco earth-tone glazes guide. Within AMACO, the darker crystal glazes CO-7 Solar Flare and CO-8 Dark Star belong to the Cosmos line; our AMACO Cosmos review covers them, including the decorative-only food label.
Safety notes
Read AMACO's SDS for each color before use. Brush rather than spray. Wet-clean spills and dust instead of sweeping, because glaze and clay dust contain silica. Mixing a dry dipping mix means handling powder: wear a NIOSH-approved respirator and wet the area afterward. Follow your kiln maker's clearance and ventilation rules for every glaze firing.
Sources: AMACO shop pages for PC-67 River Rock, PC-15 Satin Oribe, PC-25 Textured Turquoise, PC-56 Ancient Copper, PC-63 Cosmic Tea Dust, PC-10 June Bug, PC-65 Black Aventurine, C-27 Storm and C-49 Rainforest; AMACO Potter's Choice product sheet and FAQ; AMACO PC-67 River Rock layering chart; AMACO 2019 field guide Potter's Choice page; AMACO layering library entries; AMACO blog posts "Customer Favorite AMACO Glaze Combinations to Try" and "Great Glaze Combos to Try Out in 2026"; dealer listings at The Ceramic Shop, Krueger Pottery and 1240.design. Specs checked November 2026.