Verdict
Mayco Winter Wood is the most distinctive glaze in this group and the one Mayco supports best, with a 12-glaze combination sheet and a named base glaze for softer crystals. It needs care: the brown crystals settle in the jar and flow more than the base, so how you stir and where you brush decides the result. If you want brown without crystal handling, Tiger's Eye is the easiest, since Mayco says it will not run off the ware. Smoke and Amber Quartz are quiet breaking glazes that show texture, and Black Timber is a darker crystal brown.
All five Stoneware glazes here carry Mayco's dinnerware label and the ACMI AP seal. Crackerjack Brown is different: it is a cone 06 Stroke & Coat glaze that only turns streaky and light at cone 6. This guide is research-based, built from Mayco's product pages, its Glazes + Engobes User Guide (revised April 2026), combination sheets and update notices, plus US dealer listings, in November 2026. We did not fire these glazes ourselves.
All six glazes at a glance
| Glaze | Code and type | Cone | Finish (Mayco) | Coats | Food label (Mayco) | Light vs dark clay |
|---|---|---|---|---|---|---|
| Winter Wood | SW-155, Stoneware Crystal | Shown at 5, 6 ox and 10 red | Matte white with melting brown crystals | Chips at 1 to 4; no count stated | Dinnerware safe, ACMI AP | Chips on white only |
| Smoke | SW-121, Stoneware classic | Shown at 5, 6 ox and 10 red | Opaque gray-blue, soft variegation | 1 to 3, each changes the look | Dinnerware safe, ACMI AP | Samples on speckled white, speckled brown, dark clay; not described |
| Black Timber | SW220, Stoneware Crystal | Shown at 5, 6 ox and 10 red | Satin, opaque mottled brown with glossy brown crystals | Chips at 1 to 4; no count stated | Dinnerware safe, ACMI AP | Shown on five clays; not described |
| Amber Quartz | SW-173, Stoneware matte | Shown at 5, 6 ox and 10 red | Warm amber matte with tan and brown | Thick is even; thin breaks | Dinnerware safe, ACMI AP | Samples on speckled and dark clay; not described |
| Tiger's Eye | SW-112, Stoneware classic | Shown at 5, 6 ox and 10 red | Glossy deep red-brown to frothy amber | 1 to 2 for browns and reds; 3 to 5 for movement | Dinnerware safe, ACMI AP | Samples on speckled and dark clay; not described |
| Crackerjack Brown | SC-25, Stroke & Coat | 06 to 10; made for 06 | Gloss brown at 06; semi-transparent, streaky at 6 | 1 translucent; 2 to 3 opaque | Dinnerware icon; AP per Mayco's Stroke & Coat sheet | Chips on white only |
Stoneware labels come from the table in Mayco's 2026 user guide. Mayco's Stoneware brochure gives the line's range as cone 5 to 10, 2,185°F to 2,381°F (1,196°C to 1,305°C). Stoneware pints typically run about $12 to $17 at the US dealers we checked in November 2026; check the live price.
Mayco Winter Wood (SW-155)
Mayco describes Winter Wood at cone 6 oxidation as a matte white with brown crystals that melt during firing. At cone 10 reduction the color shifts to a translucent golden brown. Mayco also shows soda and wood fired results and says those vary, and that fired results depend on how the piece sits in the kiln.
- Sizes: SW-155 pint; SD-155 10 lb dry
- Base glaze: SW-106 Alabaster
- Label: dinnerware safe, ACMI AP
- Coats: chips at one to four coats; Mayco's line advice is two to four
How to handle Winter Wood's crystals
- Stir from the bottom with a palette knife or other unpainted tool before first use, and again between coats, because the crystals settle.
- Keep heavy crystal areas out of the bottom third of vertical pieces, since crystals flow more than the base glaze.
- While each coat is wet, spread the crystals evenly with a fan brush.
- Do not pile on crystals: Mayco says a heavy load can cause pinholing or running.
- Store the jar upside down so the crystals mix in more easily next time.
For a lighter crystal effect, Mayco suggests two coats of SW-106 Alabaster followed by a third coat of Winter Wood. Alabaster is covered with Mayco's other speckled whites in our Mayco speckled glazes guide. For dry crystal glazes, Mayco's user guide recommends pouring rather than dipping, to control where the crystals land.
Mayco reformulated Winter Wood in late 2021 after a talc it used (AmTalc 98) was discontinued, and said in February 2022 that the change "has slightly changed the fired result". One UK dealer, Bath Potters, adds that the wet glaze shifted from gray to buff. Older photos online may not match a new jar.
Winter Wood combinations from Mayco
Mayco's Winter Wood sheet uses two coats of Winter Wood as the base under two coats of each of these, at cone 6 and cone 10: SW-150 Celadon Bloom, SW-108 Green Tea, SW-121 Smoke, SW-206 Melon, SW-251 Pink Opal, SW-252 Blue Opal, SW-109 Capri Blue, SW-131 Birch, SW-112 Tiger's Eye, SW-119 Cinnabar, SW-177 Raspberry Mist and SW-111 Wrought Iron. Mayco's combination database also lists Winter Wood on top of SW-143 Abalone, SW-166 Norse Blue, SW-190 Passion Flower and SW-115 Midnight Rain, and the product page shows it over and under SW-401 Light Flux and SW-402 Dark Flux.
Who should skip it: anyone who wants a predictable, even surface across a matching set, and beginners who will not stir between coats.
Mayco Smoke (SW-121)
Smoke is a Stoneware classic glaze. At cone 6 oxidation Mayco calls it "an opaque grey-blue stoneware glaze with soft, subtle variegating hues", with brown breaking on raised surfaces. At cone 10 reduction it changes to a variegated sage green with a glossy finish, so the same jar gives two quite different glazes. Mayco's user guide rates it stable.
- Sizes: SW-121 pint; SD-121 10 lb dry
- Coats: one coat gives a blue-gray haze over a weathered brown; two intensify the gray; three give the full gray-blue opaque finish
- Label: dinnerware safe, ACMI AP
- Layering: over and under Light Flux and Dark Flux at cone 6; under them at cone 10 reduction; on top of Winter Wood (Winter Wood sheet)
Because thickness changes the color so much, keep coats even on a set of mugs. For Mayco's brighter blues, see our Mayco blue and green glazes guide.
Who should skip it: cone 10 potters who want gray, since reduction turns it sage green, and anyone who wants a strong blue.
Mayco Black Timber (SW220)
Black Timber is a Stoneware crystal glaze. Mayco describes a satin, opaque, mottled brown that breaks over texture at cone 6 oxidation, with glossy brown crystals that can create movement while the base stays stable. At cone 10 reduction it turns darker and more metallic and the crystals flow more, so Mayco recommends a light application there.
- Sizes: SW220 pint; SD220 10 lb dry
- Base glaze: SW144 Lava Rock, which Mayco's guide marks discontinued
- Label: dinnerware safe, ACMI AP
- Layering: over and under SW-401 Light Flux and SW-402 Dark Flux at cone 6 and cone 10
Crystal handling is the same as Winter Wood: stir thoroughly with an unpainted tool, keep crystals off the bottom third of tall forms, spread them with a fan brush and avoid heavy crystal loads, which Mayco links to pinholing and running. Because its base glaze is discontinued, you cannot copy Mayco's lighter crystal method the way you can with Winter Wood.
Who should skip it: cone 10 reduction potters who glaze heavily, and anyone who wants a near black; despite the name, Mayco describes a mottled brown.
Mayco Amber Quartz (SW-173)
At cone 6 oxidation Mayco describes a warm amber matte with accents of tan and brown. Thick coats give a more even color; thin areas break translucent and pool darker around texture. At cone 10 reduction it turns glossy, and purple and blue show more. Mayco's guide says matte Stoneware glazes need at least cone 6 for a smooth satin matte, so do not underfire it.
- Sizes: SW-173 pint only; the SD-173 dry version was discontinued on January 1, 2023, while the pint stayed
- Label: dinnerware safe, ACMI AP
- Layering: over and under Light Flux and Dark Flux at cone 6; under them at cone 10; on top of SW250 White Opal and SW229 Mood Ring (Mayco's sheets for those glazes)
Both of those base glazes are covered in our Mayco Micro and Opal glazes guide.
Who should skip it: dipping studios, since there is no dry version, and cone 10 potters who want the matte amber look.
Mayco Tiger's Eye (SW-112)
Mayco says Tiger's Eye breaks from a glossy deep brownish red to a frothy amber at cone 6, depending on thickness. One to two coats give browns and reds; three to five give more movement and color variation, yet Mayco states it "will not run off your ware". Thinner coats fire darker brown and red, heavier coats lean toward an opaque light brown. At cone 10 the color darkens.
- Sizes: SW-112 pint; SD-112 10 lb dry
- Label: dinnerware safe, ACMI AP
- Layering: over and under Light Flux and Dark Flux at cone 6; on top of Winter Wood and Opal Lustre (Mayco's sheets); Mayco names SW-104 Black Walnut as a complementary glaze
Mayco also says that when Tiger's Eye is butted against another glaze it gently merges with it, which makes it a good band or rim glaze next to a matte.
Who should skip it: anyone who wants a matte or a cool-toned brown.
Mayco Crackerjack Brown (SC-25), a Stroke & Coat glaze
Crackerjack Brown is not a Stoneware glaze. Mayco lists it as SC-25 (written SC-025 on its page) in the Stroke & Coat line: a heavily pigmented, viscous cone 06 glaze for brush strokes or opaque coverage that fires glossy without a clear coat. One coat is translucent and two to three give full opacity. At cone 6 Mayco says it turns semi-transparent and streaky, and the color lightens to "a slightly darker SC-5 Tiger Tail". It comes in 2 oz and 8 oz squeeze bottles and pints, and Mayco includes it in Stroke & Coat Kit #2 (check the kit on Amazon).
The product page shows a dinnerware icon, and Mayco's Stroke & Coat consumer information sheet applies the ACMI AP seal to the line. How the line works on greenware and bisque is on our Mayco Stroke and Coat page.
Who should skip it: cone 6 potters who want a solid brown; use one of the Stoneware browns above instead.
Black Walnut, the other Mayco brown
SW-104 Black Walnut is Mayco's dark brown soft matte, which Mayco says needs four or more coats for full color. It has its own page: see our Mayco Black Walnut glaze review.
Earth tones on light and dark clay
Mayco fires its chips flat on white clay and says clay body, thickness, firing and temperature all change the result. It shows Smoke, Amber Quartz and Tiger's Eye on speckled white, speckled brown and dark clay, and Black Timber on five clays, but it does not describe those results in words. Expect breaking glazes like Smoke and Amber Quartz to look darker and warmer on brown bodies, and test first. Our dark clay bodies page explains why.
How to apply these glazes
Mayco's user guide says to load a soft fan brush (RB-144 or RB-140), let the excess drip off and brush two to four coats on bisque, drying between coats; thrown and handbuilt work typically needs three coats. Mayco recommends a single dip of dry glaze mixed with distilled water to package directions, and pouring for dry crystal glazes. Fire to cone 6 with a witness cone, and leave room for movement on vertical tests. Our how to glaze pottery guide covers brushing and dipping.
Dry glaze contains silica. Wear a NIOSH-approved respirator when mixing powder, wet-wipe spills and never dry sweep. Read Mayco's SDS for each line before use.
Food labels, in plain terms
Winter Wood, Smoke, Black Timber, Amber Quartz and Tiger's Eye are listed as dinnerware safe with the ACMI AP seal in Mayco's 2026 guide. Mayco says it has not tested every combination, so layered results cannot be certified, and makers selling food-contact ware must test their own pieces.
We cannot promise any glaze is food safe on your pots. Results depend on firing to the stated cone, on your clay and on testing.
What this group does well
- Every Stoneware glaze here carries a dinnerware label.
- A real range: white with brown crystals, gray-blue, mottled brown, amber and red-brown.
- Clear crystal handling advice and a 12-glaze Winter Wood combination sheet.
Weak points
- Winter Wood and Black Timber need stirring between coats and careful placement.
- Smoke and Amber Quartz look very different at cone 10.
- Amber Quartz has no dry version, and Black Timber's base glaze is discontinued.
Who should buy and who should skip
Buy Winter Wood or Black Timber if you like crystal streaks and will stir and test. Buy Tiger's Eye or Smoke for low-risk breaking glazes on functional ware, and Amber Quartz for a warm matte at cone 6. Skip this group if you fire low fire only, except Crackerjack Brown.
Alternatives
- For the full cone 6 line and Mayco's Flux layering, see our Mayco Stoneware glazes review.
- For an overview of every Mayco line, see the Mayco glazes review.
Sources: Mayco product pages for SW-155 Winter Wood, SW-121 Smoke, SW220 Black Timber, SW-173 Amber Quartz, SW-112 Tiger's Eye and SC-25 Crackerjack Brown; Mayco Glazes + Engobes User Guide (revised April 2026); Mayco combination sheets for SW-155, SW-219 and SW-250, and its Glaze Combinations database; Mayco Product Updates page (2021 and 2022 reformulation notes, 2023 dry discontinuations); Mayco Stroke & Coat Consumer Product Information Sheet; Mayco Stoneware brochure; dealer listings at Bath Potters, Ceramic Superstore and BuyMayco. Specs checked November 2026.