Verdict
If you want one glaze from this group for mugs and bowls, Mayco Micro Pearl is the safe start: it is the only Micro glaze with a dinnerware label, it is stable at three coats, and it shows a pearly lilac shimmer at cone 6. White Opal and Pink Opal are calm, glossy picks for functional ware. Micro Cerulean, Micro Jade and Mood Ring are the showpieces, but Mayco labels all three not dinnerware safe, and two of them move at three coats.
Opal Lustre is a cone 6 glaze, not a metallic luster, and Mystic Jade and Copper Adventurine are low fire glazes from other Mayco lines. This guide is research-based, built from Mayco's product pages, user guide, combination sheets and update notices plus US dealer listings in November 2026. We did not fire these glazes ourselves.
All nine glazes at a glance
| Glaze | Code and line | Cone | Finish (Mayco) | Coats | Food label (Mayco) | Light vs dark clay |
|---|---|---|---|---|---|---|
| Micro Pearl | SW-214, Stoneware (Micro) | Shown at 5, 6 ox and 10 red; crystals best at 6 ox | Glossy, semi-opaque white with lilac undertones | Stable at 3 | Dinnerware safe, ACMI AP | Shown on five clays; not described |
| Micro Cerulean | SW-217, Stoneware (Micro) | Same as Micro Pearl | Glossy, translucent medium blue with an aqua float | Stable at 3 | Not dinnerware safe, ACMI CL | As Micro Pearl |
| Micro Jade | SW-216, Stoneware (Micro) | Same as Micro Pearl | Glossy, translucent green with a turquoise float | Fluid at 3; apply less | Not dinnerware safe, ACMI CL | As Micro Pearl |
| Opal Lustre | SW-219, Stoneware classic | Shown at 5, 6 ox and 10 red | Glossy, semi-opaque blue, green and purple | Semi-fluid at 3 | Dinnerware safe, ACMI AP | Shown on five clays; not described |
| White Opal | SW-250, Stoneware classic | Shown at 5, 6 ox and 10 red | Clear to milky white gloss | 1 coat clearest; more coats add white | Dinnerware safe, ACMI AP | Mayco: white shows more on darker bodies |
| Pink Opal | SW-251, Stoneware classic | Shown at 5, 6 ox and 10 red | Desert rose pink gloss | Thin is clear; thick is opaque purple-pink | Dinnerware safe, ACMI AP | Chips on white only |
| Mood Ring | SW-229, Stoneware classic (2026) | Shown at 5, 6 ox and 10 red | Glossy, opaque dark green breaking brown | Semi-fluid at 3 | Not dinnerware safe, ACMI CL | Shown on six clays; not described |
| Mystic Jade | CG-780, Jungle Gems | 06; also shown at 6 ox | Semi-translucent blue-green with jade and brown crystals | Not on the product page | Not dinnerware safe | Not published by the maker |
| Copper Adventurine | EL-121, Elements | 06; also shown at 6 ox and 10 red | Glossy, metallic dark brown and copper with a yellow stain | Not on the product page | Not dinnerware safe | Not published by the maker |
Labels come from Mayco's 2026 user guide table, or the product page icon for the two low fire glazes. Mayco's Stoneware brochure gives the line's range as cone 5 to 10, 2,185°F to 2,381°F (1,196°C to 1,305°C). Pints typically run about $12 to $17 at the US dealers we checked in November 2026, and 10 lb dry bags around $100 to $110 where still sold; check the live price.
What Mayco means by Micro and Opal
The Micro glazes arrived in Mayco's 2024 Stoneware release. Mayco describes "micro-crystallization" that develops during firing and recommends cone 6 oxidation for it. Krueger Pottery, a dealer, explains that the small crystals form from zinc and silica as the glaze cools, and may not form at higher temperatures, which fits Mayco's variegated cone 10 chips. For true crystal firing with controlled cooling, see our crystalline glaze guide.
The Opal names are Stoneware classic glosses that break and pool over texture. They need no extra firing.
Mayco's 2026 discontinuation list drops the 10 lb dry versions of Micro Jade (SD216), Micro Cerulean (SD217), Micro Ash (SD218), Opal Lustre (SD219) and Pink Opal (SD251), plus Micro Champagne in both pint (SW215) and dry. Mayco says to buy "while supplies last". The other pints still have live product pages in November 2026.
Mayco Micro Pearl (SW-214)
At cone 6 oxidation, Mayco describes Micro Pearl as a glossy, semi-opaque white with lilac undertones that breaks over texture, with iridescent micro-crystals in lilac and pale yellow. At cone 5 it stays a stable, frosted white with a pearlescent satin finish. At cone 10 reduction it darkens to a blue, purple and white variegation.
- Sizes: SW-214 pint; SD-214 10 lb dry
- Coats: stable at 3; more coats or a thicker layer "may result in movement"
- Label: dinnerware safe, ACMI AP
- Layering shown by Mayco: over and under SW-401 Light Flux and SW-402 Dark Flux
Mayco's product page calls Micro Pearl semi-opaque at cone 6; its user guide table says "Opaque".
Micro Pearl combinations from Mayco
Mayco's sheet puts two coats of each of these over two coats of Micro Pearl: SW-165 Lavender Mist, SW-193 Ivy, SW-215 Micro Champagne, SW-218 Micro Ash, SW-108 Green Tea, SW-189 Cenote, SW-199 Purple Aster, SW-217 Micro Cerulean, SW-184 Speckled Toad, SW-194 Nimbus, SW-216 Micro Jade and SW-219 Opal Lustre, at cone 6 and cone 10 reduction. The Opal Lustre sheet also uses Micro Pearl as a top coat.
Who should skip it: cone 10 only potters, since Mayco ties the crystals to cone 6 oxidation, and anyone wanting a flat, solid white.
Mayco Micro Cerulean (SW-217)
Micro Cerulean fires at cone 6 oxidation to a glossy, translucent medium blue with an aqua float that breaks over texture, with blue micro-crystal blooms. At cone 5 Mayco shows a stable, semi-opaque deep blue with a pearlescent satin finish, and at cone 10 reduction a variegated gray-blue. Because it is translucent, Mayco asks for an even application so brush strokes do not fire streaky.
- Sizes: SW-217 pint; SD-217 dry is on the 2026 discontinuation list
- Coats: stable at 3; thicker may move
- Label: not dinnerware safe, ACMI CL
- Layering shown by Mayco: over and under SW-401 Light Flux and SW-402 Dark Flux; on top of Micro Pearl
For other Mayco blues such as Tropical Teal and Norse Blue, see our Mayco blue and green glazes guide.
Who should skip it: anyone who wants a blue for the inside of mugs or plates, and brushers who struggle with even coats, since translucent blues show every stroke.
Mayco Micro Jade (SW-216)
Micro Jade fires at cone 6 oxidation to a glossy, translucent green with a turquoise float and bronze micro-crystal blooms. At cone 5 Mayco shows a stable, semi-opaque olive with a pearlescent satin finish that breaks over texture, and at cone 10 reduction it turns a variegated brown. This is the runniest of the three Micros: Mayco calls it fluid at three coats and says to apply less to avoid runoff.
- Sizes: SW-216 pint; SD-216 dry is on the 2026 discontinuation list
- Coats: fluid at 3; use fewer or thinner coats
- Label: not dinnerware safe, ACMI CL
- Layering shown by Mayco: over and under Light Flux and Dark Flux; on top of Micro Pearl
Taper Micro Jade toward the foot and fire your first test on a catch tile.
Who should skip it: beginners without spare kiln shelves or catch tiles, and anyone glazing food surfaces.
Mayco Mystic Jade (CG-780), a Jungle Gems glaze
Mystic Jade is not a Micro glaze. Mayco lists it as CG-780 in the Jungle Gems crystal glaze line, fired at cone 06: a semi-translucent blue-green base glaze with variegated jade and brown crystals. At cone 6 oxidation the base darkens and the crystals turn opaque brown. Mayco notes enhanced mobility and possible surface issues, shows a not dinnerware safe icon, and sells 4 oz and pint sizes. Coats and crystal handling are on our Mayco Jungle Gems page.
Who should skip it: cone 6 potters who want Micro Jade's look; the two names are similar, but the lines and firings are not.
Mayco Opal Lustre (SW-219)
Opal Lustre fires at cone 6 oxidation to a glossy, semi-opaque glaze with blue, green and purple variation that breaks warm brown over texture. At cone 10 reduction Mayco says the color flattens and warm undertones come through. Mayco calls it semi-fluid at three coats, and its user guide rates it "Fluid", so more coats can move.
- Sizes: SW-219 pint; SD-219 dry is on the 2026 discontinuation list
- Label: dinnerware safe, ACMI AP
- Layering: over and under Light Flux and Dark Flux; Mayco's combination sheet uses two coats of Opal Lustre under SW-101 Stoned Denim, SW-148 Lime Shower, SW-199 Purple Aster, SW-203 Root Beer, SW-112 Tiger's Eye and SW-214 Micro Pearl, on white stoneware and on several Mayco engobes
Mayco added a 2024 jar notice about varied results, and in June 2024 pulled pint lot 2407077 for firing darker with less variation. Test each new jar.
Despite the name, it is fired once like any glaze, with no metallic overglaze layer. For real lusters, see our gold glaze for ceramics guide.
Who should skip it: potters who need repeatable color across a set, given Mayco's own variability notice, and anyone who wants a pearly metallic sheen; it is a gloss with color breaks, not a luster.
Mayco White Opal (SW-250)
White Opal fires at cone 6 oxidation to a clear to milky white gloss. Mayco says "one coat produces the clearest finish", extra coats add white precipitate, and white to bluish-white shows where the glaze pools around texture. At cone 10 reduction there is less white variation, leaving a transparent gloss with white pooling. It is one of the few glazes here where Mayco describes clay color: white shows more on darker bodies such as Buff and Manganese Speck.
- Sizes: SW-250 pint; SD-250 10 lb dry (not on the 2026 list)
- Label: dinnerware safe, ACMI AP
- Layering: Mayco's combination sheet uses two coats of White Opal under SW-130 Copper Jade, SW-164 Satin Patina, SW-173 Amber Quartz, SW-192 Amaryllis, SW-129 Copper Float, SW-146 Aurora Green, SW-167 Sand & Sea, SW-184 Speckled Toad, SW-132 Mirror Black, SW-165 Lavender Mist, SW-183 Oxblood and SW-194 Nimbus
Who should skip it: anyone who wants a solid opaque white; White Opal is closer to a soft, pooling clear.
Mayco Pink Opal (SW-251)
Mayco calls Pink Opal a desert rose pink at cone 6 oxidation. Thin areas fire clear with hints of pink, heavier areas fire opaque purple-pink with a gloss, and some spots show a whitish cast. On vertical pieces it flows into a semi-transparent rose veil, and texture stays visible unless the glaze is thick. At cone 10 reduction the pink fades out, leaving a transparent gloss with white pooling, so this is a cone 6 color.
- Sizes: SW-251 pint; SD-251 dry is on the 2026 discontinuation list
- Label: dinnerware safe, ACMI AP
- Layering: Mayco's sheet uses two coats of Pink Opal under SW-109 Capri Blue, SW-135 Wintergreen, SW-153 Indigo Rain, SW-189 Cenote, SW-104 Black Walnut, SW-128 Cordovan, SW-146 Aurora Green, SW-185 Rain Forest, SW-110 Oyster, SW-145 Tea Dust, SW-156 Galaxy and SW-203 Root Beer
Mayco flagged pint lot 2411046 in May 2024 as not performing to its standards, so check lot numbers on older stock.
Who should skip it: cone 10 reduction potters, and anyone wanting a strong, even pink; this one is a pale, pooling rose.
Mayco Mood Ring (SW-229)
Mood Ring is part of Mayco's 2026 Stoneware release. At cone 6 oxidation Mayco describes "a glossy, opaque dark green glaze that breaks brown over texture" with an iridescent sheen. At cone 10 reduction the color darkens, and heavier reduction may add surface texture. It is semi-fluid at three coats.
- Sizes: SW-229 pint; SD-229 10 lb dry
- Label: not dinnerware safe, ACMI CL
- Layering: Mayco's June 2026 sheet uses two coats of Mood Ring under SW-118 Sea Salt, SW-176 Sandstone, SW-195 Riptide, SW-408 White Flux, SW-153 Indigo Rain and SW-173 Amber Quartz, on white stoneware and on Mayco's engobes
Sea Salt and Sandstone are speckled glazes covered in our Mayco speckled glazes guide.
Who should skip it: anyone making functional ware, and households with children 12 and under, since Mayco says CL products should not be used by that age group.
Mayco Copper Adventurine (EL-121), an Elements glaze
Copper Adventurine is EL-121 in Mayco Elements, a cone 06 line made to look like mid-range glazes. At cone 06 Mayco describes a glossy, metallic dark brown and copper glaze with a yellow stain. At cone 6 oxidation it darkens to a sparkly black that breaks over texture and pools brown and red. Mayco notes enhanced mobility, possible surface issues, and that it is not overglaze compatible. It comes in 4 oz and pint, at about $5 to $7 and $16 to $19 at the dealer we checked.
The product page shows a not dinnerware safe icon. Coats, firing at cone 6 and the full Elements label list are on our Mayco Elements glazes page.
Who should skip it: potters who want a real copper metal surface, and anyone glazing food surfaces.
How to apply these glazes
Mayco's user guide says to load a soft fan brush (it names RB-144 and RB-140), let the excess drip off, and brush two to four coats on bisque, drying between coats. Thrown and handbuilt work typically needs three coats, slip cast work two.
- Brush full, even coats; translucent Micros show streaks if coats vary.
- Stop at two coats for Micro Jade, Opal Lustre and Mood Ring on vertical walls until you have tested three.
- Fire to cone 6 oxidation with a witness cone, and test vertically, since Mayco warns extra heat makes glazes more fluid.
For dipping, Mayco says to mix dry SD glazes thoroughly with distilled water to the package directions, and recommends a single dip to match its sample tiles. Only Micro Pearl, White Opal and Mood Ring still have dry versions off the 2026 list. Our how to glaze pottery guide covers brushing and dipping in more detail.
Dry glaze contains silica. Wear a NIOSH-approved respirator when mixing powder, wet-wipe and mop spills, and never dry sweep. Read Mayco's Stoneware SDS before use, and keep fluid glazes off kiln shelves with a catch tile.
Food labels, in plain terms
Four glazes here carry Mayco's dinnerware label and the ACMI AP seal; the rest do not (see the table). Mayco says it has not tested every combination, so layered results cannot be certified, and a clear coat over a not dinnerware safe glaze does not make it dinnerware safe.
We cannot promise any of these glazes is food safe on your pots. Results depend on firing to the stated cone, on your clay, and on testing.
What this group does well
- Clear food labels for each glaze, published in one table in Mayco's guide.
- Three distinct looks at one cone: shimmer, pooling gloss and iridescent green.
- Published combination sheets for five of the glazes.
Weak points
- Three of the seven Stoneware glazes here are not dinnerware safe.
- Micro Jade, Opal Lustre and Mood Ring move at three coats.
- Most dry versions are being dropped in 2026.
- Mayco shows dark clay samples but rarely describes them in words.
Who should buy and who should skip
Buy Micro Pearl, White Opal or Pink Opal for glossy cone 6 functional ware with texture. Buy Micro Cerulean, Micro Jade or Mood Ring for vases, planters and pot exteriors. Skip the Micros if you fire only cone 10, and skip this group if you fire only low fire.
Alternatives
- For a stable, all-round cone 6 palette, our Mayco Stoneware glazes review covers the whole line.
- For an overview of every Mayco line, from Stroke & Coat to Stoneware, see the Mayco glazes review.
- For more cone 6 options from other brands, see our cone 6 glazes guide.
Sources: Mayco product pages for SW-214 Micro Pearl, SW-216 Micro Jade, SW-217 Micro Cerulean, SW-219 Opal Lustre, SW-250 White Opal, SW-251 Pink Opal, SW-229 Mood Ring, CG-780 Mystic Jade and EL-121 Copper Adventurine; Mayco Glazes + Engobes User Guide (revised April 2026); Mayco combination sheets for SW-214, SW-219, SW-250, SW-251 and SW-229; Mayco 2026 Stoneware Release page; Mayco Product Updates page (2024 notices and 2026 discontinuations); Mayco Stoneware brochure; dealer listings at Krueger Pottery, Seattle Pottery Supply and Stoneleaf Pottery. Specs checked November 2026.