Verdict
Mayco Tropical Teal is the easiest pick in this group for a home potter with a cone 6 electric kiln: Mayco calls it stable, it shows texture without heavy movement notes, and it carries the Dinnerware Safe mark on its product page. If you want more drama, the crystal glazes (Blue Splatterware, Blue Hydrangea and Olive Float) bloom at cone 6 but need stirring, careful placement and test tiles.
The nine glazes on this page come from three different Mayco lines, and that matters more than the color. Five are cone 6 Stoneware glazes, two are low fire Elements, and two are Stroke & Coat colors that fire from cone 06 to 10. This guide is research-based: we compared Mayco's product pages, line pages, its 2023 Stroke & Coat brochure and its 2026 Color Guide, plus dealer listings for prices. We did not fire these glazes.
For how the Mayco lines fit together, see our Mayco glazes review.
The nine glazes at a glance
| Glaze | Code and line | Cone (Mayco) | Finish | Coats | Food label (Mayco page) | Light vs dark clay (Mayco) |
|---|---|---|---|---|---|---|
| Tropical Teal | SW224, Stoneware | 6 ox, 10 red | Gloss, semi-opaque, mottled float | 1 to 4 shown; 1 shows the clay | Dinnerware Safe | Shown on white, speckled, red, dark brown and black clay |
| Norse Blue | SW-166, Stoneware | 6 ox, 10 red | Gloss, semi-opaque | 1 to 3 shown; thicker is more even | Dinnerware Safe | Shown on speckled white, speckled brown and dark clay |
| Blue Splatterware | SW-152, Stoneware crystal | 6, 10 red | Semi-matte white with blue blooms | No count; 1 to 4 shown | Dinnerware Safe | Shown on speckled white, speckled brown and dark clay |
| Blue Hydrangea | SW-170, Stoneware crystal | 6, 10 | Blue with white and yellow blooms | No count; 1 to 4 shown | Dinnerware Safe | Shown on speckled white, speckled brown and dark clay |
| Olive Float | SW-151, Stoneware crystal | 6 ox, 10 red | Dark green gloss, light green crystal | No count; 1 to 3 shown | Dinnerware Safe logo | Shown on speckled white, speckled brown and dark clay |
| Stormy Blue | EL-124, Elements | 06 (changes at 6) | Matte metallic silver and blue | Not stated | Not dinnerware safe | Not published |
| Mirror Blue | EL-134, Elements | 06 (darkens at 6) | Glossy vibrant blue | Semi-transparent at 3 | Not dinnerware safe | Not published |
| Moody Blue | SC-12, Stroke & Coat | 06 to 10 | Gloss without clear | 2 to 3 for opacity | Dinnerware Safe | Chips on white clay only |
| Irish Luck | SC-36, Stroke & Coat | 06 to 10 (line) | Gloss without clear (line) | 2 to 3 for opacity (line) | Line labeled Dinnerware Safe | Not published for this color |
Price band: a pint of a Mayco Stoneware glaze typically runs about $13 to $18 at US dealers in November 2026, and a 10 lb dry bag (SD code) sits around $100 to $110 at the dealer we checked. Elements run about $5 to $17 depending on jar size, and Stroke & Coat about $4 to $7 for 2 oz. Check the live price.
Mayco Tropical Teal (SW224)
Mayco describes Tropical Teal as "a glossy, semi-opaque teal glaze with a mottled float that breaks over texture," and adds that the glaze is stable. At cone 10 reduction it shows an enhanced green undertone. Mayco says the blue gets stronger as the coat gets thicker, so a thin coat reads greener and a heavy coat bluer.
Light and dark clay: Mayco shows cone 6 oxidation tiles on white, speckled, red, dark brown and black clay, which is wider than most of its pages. Its general Stoneware note is that one coat lets the clay body show through and two to three coats deepen the color, so on a dark body plan on at least two coats if you want the teal to read as teal.
Application: Mayco does not state brushing or dipping on the product page. It sells a pint for brushing and SD224, a 10 lb dry bag, for mixing a dipping bucket. Mayco's sample tiles run from one to four coats.
Layering: Mayco shows Tropical Teal over and under SW-401 Light Flux and SW-402 Dark Flux at cone 6 oxidation and cone 10 reduction. Those two fluxes get their own page at Mayco flux glazes.
- Code: SW224 pint; SD224 10 lb dry
- Cone: 6 oxidation and 10 reduction; stable at both per Mayco
- Finish: gloss, semi-opaque, mottled float
- Label: Dinnerware Safe mark and ACMI seal
Pros
- Stable with no movement warning
- Shows texture
- Tested by Mayco on dark and red clay too
Cons
- Color shifts between blue and green with thickness
- No published coat count
Who should skip it: low fire potters at cone 06, and anyone who needs an exact color match across a set.
Mayco Norse Blue (SW-166)
Norse Blue is a semi-opaque blue gloss with light blue and green tones. Mayco says the look depends on application: thicker coats look more even, while thinner areas break translucent and pool darker over texture. Cone 10 reduction darkens the color. Mayco shows no movement warning for it.
Light and dark clay: Mayco fires the main chips flat on a white clay body and shows extra cone 6 tiles on speckled white, speckled brown and dark clay. Because thin spots break translucent, the clay color will show on rims and edges, more so on a dark body.
Application and sizes: Mayco lists a pint, a gallon and SD-166 10 lb dry, so Norse Blue is one of the few glazes here you can buy in a brushing gallon. The general Stoneware note of one coat to show the clay and two to three to deepen it applies.
Layering: Mayco shows Norse Blue over and under SW-401 Light Flux and SW-402 Dark Flux at cone 6, and under the fluxes at cone 10 reduction.
- Code: SW-166 pint and gallon; SD-166 10 lb dry
- Cone: 6 oxidation, 10 reduction (darker)
- Finish: gloss, semi-opaque
- Label: Dinnerware Safe mark and ACMI seal
Pros
- Calm, even blue at thicker coats
- Gallon size
- No movement warning
Cons
- Thin areas go translucent, so uneven brushing shows
Who should skip it: potters who want crystals or a matte surface.
How Mayco's crystal glazes behave
Blue Splatterware, Blue Hydrangea and Olive Float all hold crystals in a base glaze, and Mayco prints the same handling rules on each page. These rules matter more than coat count:
- Stir thoroughly before first use, because the crystals settle in the jar. Mayco says to use a palette knife or another unpainted tool.
- Re-stir between every coat.
- While the glaze is wet, use a fan brush to spread the crystals evenly.
- Keep crystals off the bottom third of vertical pieces, since the crystals flow more than the base glaze.
- Avoid heavy crystal buildup, which Mayco says can cause pinholing or running.
- Store the jar upside down so the crystals disperse more easily next time.
Mayco also says results vary with the ware's orientation, so a flat tile and a mug wall will not match. True crystalline glazes grown in a special firing are different; see crystalline glaze.
Mayco Blue Splatterware (SW-152)
Mayco describes Blue Splatterware as "a white, semi-matte glaze that contains a blue crystal." At cone 6 the melting crystal forms small blue blooms that make the surface look like 19th century enamelware. At cone 10 the crystals become less defined.
Light and dark clay: Mayco shows cone 6 tiles on speckled white, speckled brown and dark clay but writes no light vs dark note.
Application: the page shows one to four coats and a three coat tile at cones 5, 6 and 10 reduction. Follow the crystal rules above and fan the crystals while wet.
Layering: for a lighter crystal effect, Mayco suggests two coats of SW-141 White Matte, the base glaze, then a third coat of Blue Splatterware. Mayco also shows it over and under SW-401 Light Flux and SW-402 Dark Flux. You can check SW-141 White Matte on Amazon if you want to try the lighter version.
- Code: SW-152 pint only
- Cone: 6 (oxidation and reduction tiles), 10 reduction
- Finish: semi-matte white with blue blooms
- Label: Dinnerware Safe mark and ACMI seal
Pros
- Distinctive speckled enamel look
- Named base glaze for a lighter version
Cons
- Pint only, no dry bag
- Crystals need stirring and placement care
Who should skip it: potters who glaze tall forms quickly, or fire to cone 10 and want crisp spots.
Mayco Blue Hydrangea (SW-170)
Blue Hydrangea is a blue, floral-inspired glaze with yellow and white crystals. When the crystals melt at cone 6, Mayco says large white blooms and smaller yellow blooms form. At cone 10 the color shifts toward blue and the crystals fade slightly. Mayco does not state a gloss or matte finish.
Application and clay: brush it, fanning the crystals while wet. The page shows one to four coats with no recommended count, and cone 6 tiles on speckled white, speckled brown and dark clay with no written clay note.
Layering: Mayco shows it over and under SW-401 Light Flux and SW-402 Dark Flux at cone 6 oxidation and cone 10 reduction.
- Code: SW-170 pint; SD-170 10 lb dry
- Cone: 6 and 10 (crystals fade slightly at 10)
- Finish: blue with white and yellow blooms; gloss level not stated
- Label: Dinnerware Safe mark and ACMI seal
Pros
- Large blooms
- Dry bag for dipping
Cons
- No coat count or finish stated
- Crystal handling needed
Who should skip it: anyone who wants a plain blue without spots.
Mayco Olive Float (SW-151)
Olive Float is the green anchor of the group: Mayco calls it "a dark green gloss glaze that contains a light green crystal." In cone 10 reduction it turns red and the crystals remain, which is a large change, so do not move a cone 6 favorite to a cone 10 kiln without a test.
Clay and application: chips are fired on a white body, with cone 6 tiles on speckled white, speckled brown and dark clay; Mayco says clay choice affects results. One to three coats are shown at cones 5 and 6. Pint only.
Layering: for a lighter crystal effect, Mayco suggests SW-210 Emerald as the base with Olive Float as a third coat. It also shows Olive Float with SW-401 Light Flux and SW-402 Dark Flux.
- Code: SW-151 pint
- Cone: 6 oxidation; 10 reduction (turns red)
- Finish: dark green gloss with light green crystal
- Label: Dinnerware Safe logo and ACMI seal shown
Pros
- Deep green with crystal interest
- Named base glaze
Cons
- Pint only
- Big color change at cone 10
Who should skip it: cone 10 reduction potters who want green.
Elements blues: Stormy Blue and Mirror Blue
Both are low fire Elements glazes, made for cone 06 and designed to look like mid-range glazes. Both pages warn "This glaze WILL move," tell you to thin the coat toward the bottom third of vertical pieces, and say they are not overglaze compatible. The line's coats, ramp and labels are covered on our Mayco Elements page.
Mayco Elements Stormy Blue (EL-124)
At cone 06 oxidation, Mayco describes Stormy Blue as "a matte, metallic silver and blue glaze with a mottled appearance." At cone 6 it turns a glossy yellow that breaks over texture, blue crystallization can occur, mobility increases and surface issues may occur. The product page shows a not dinnerware safe icon. Sizes are 4 oz and pint; Mayco publishes no light or dark clay note.
Pros
- Unusual metallic blue at low fire
- In the Elements kit
Cons
- Not for dinnerware
- Will move
- Changes to yellow at cone 6
Who should skip it: mug and plate makers, and cone 6 potters.
Mayco Mirror Blue (EL-134)
Mirror Blue is a glossy, vibrant blue that is semi-transparent at three coats at cone 06. At cone 6 the color darkens, mobility increases and surface issues may occur. The product page shows a not dinnerware safe icon, and our Elements page notes that Mayco's 2026 AP sheet lists it as food safe but not dinnerware safe. Sizes are 4 oz and pint.
Pros
- Bright gloss blue at low fire
- Small jar to test
Cons
- Not dinnerware safe
- Will move
- No layering named
Who should skip it: anyone glazing food surfaces.
Stroke & Coat colors: Moody Blue and Irish Luck
Stroke & Coat is Mayco's heavily pigmented brushing glaze. Mayco's 2023 brochure says one coat is translucent, two to three give full opacity, it fires glossy without a clear and it goes on wet clay, greenware or soft-fired stoneware bisque. The line has its own review at Mayco Stroke and Coat.
Mayco Moody Blue (SC-12)
Moody Blue fires to a gloss without clear at cone 06, with two to three coats for full opacity. At cone 6 oxidation Mayco notes "Semi-Transparent. Slightly moves. Color slightly lightens." It shows the Dinnerware Safe badge, and comes in 2 oz and 8 oz squeeze bottles, a pint and a gallon. Mayco also makes a speckled version, SP-212 Speckled Moody Blue, covered with the Mayco speckled glazes.
Pros
- Flat, opaque blue for designs
- Fires from cone 06 to 10
Cons
- Lighter and semi-transparent at cone 6
Who should skip it: potters after a reactive, breaking surface.
Mayco Irish Luck (SC-36)
Irish Luck is a Stroke & Coat green, listed as SC036 in Mayco's 2023 Stroke & Coat brochure, where it appears in the cone 6 results section (fired flat in oxidation on white stoneware). It also appears in Mayco's 2026 Color Guide, so it is a current color. We found no Mayco product page with a written color note for it in November 2026, so the line facts above apply: cone 06 to 10, two to three coats, and the line's Dinnerware Safe label. Utrecht's listing also shows Dinnerware Safe and the AP seal.
Pros
- A true green in an easy brushing line
- Small bottles
Cons
- No color-specific cone 6 or cone 10 note published
Who should skip it: potters who want a float or crystal green, who should look at Olive Float.
Which one fits your kiln
Cone 5 to 6 electric: Tropical Teal and Norse Blue for steady color; Blue Splatterware, Blue Hydrangea and Olive Float for crystal blooms. Our cone 6 glazes guide compares these with other brands.
Cone 06 to 05: Moody Blue and Irish Luck for opaque painted color, Stormy Blue and Mirror Blue for decorative surfaces that move.
Cone 10 reduction: test first; Olive Float turns red and Norse Blue darkens.
What these glazes do well
Every Stoneware page here shows coat tiles, cone 6 and cone 10 results and flux pairings, and the seven Stoneware and Stroke & Coat colors carry Dinnerware Safe marks. The range runs from flat brushing blue to floated teal to bloomed crystals.
Weak points
- Coat counts are missing on the crystal pages.
- Crystal handling adds steps: stirring, fanning, placement.
- Two Elements colors are not dinnerware safe and will move.
- Several glazes are pint only, with no dry bag for dipping.
Alternatives
For AMACO's cone 5 to 6 blue floats, see AMACO blue float glazes, and for its layering line, AMACO Potter's Choice. For low fire crystal bursts from Mayco, Jungle Gems are the next step. Mayco's browns and neutrals sit on the Mayco earth tone glazes page.
Safety notes
Read Mayco's SDS and product label before use. Dry SD bags release silica dust: mix them wearing a NIOSH-approved respirator, wet-clean spills and never dry sweep. Mayco says its Food Safe and Dinnerware Safe labels apply to the fired glaze used as directed, and that people who sell finished ware are responsible for testing it. Whether a glaze is safe on your own pots depends on firing to the stated cone on a suitable clay and on testing; we never promise it.
Sources: Mayco product pages SW224 Tropical Teal, SW-166 Norse Blue, SW-152 Blue Splatterware, SW-170 Blue Hydrangea, SW-151 Olive Float, EL-124 Stormy Blue, EL-134 Mirror Blue and SC-12 Moody Blue; Mayco Stroke & Coat and Stoneware line pages; Mayco Stroke & Coat brochure, mid and high fire (2023); Mayco 2026 Color Guide; Mayco Dinnerware and Food Safety page; Krueger Pottery and Utrecht dealer listings; Seattle Pottery Supply listing for price band. Specs checked November 2026.