Verdict in brief

Spectrum Bougainvillea (1447) is a cone 4/6 glaze from Spectrum's 1430 Floating line: a pink glaze that breaks into violet, purple and coral from one jar. Kimchi (1436), Sangria (1435), Shallot (1448), Sunrise (1446) and Tiger Eye (1444) are warm colors in the same line, brushed in two to three coats. Spectrum Gold (1112) is a separate metallic with a caution label and no dinnerware wording we could find.

On this page
  1. Verdict
  2. The seven warm Spectrum glazes at a glance
  3. How the warm floating glazes behave
  4. Spectrum Bougainvillea glaze (1447)
  5. Spectrum Kimchi glaze (1436)
  6. Spectrum Sangria glaze (1435)
  7. Shallot, Sunrise and Tiger Eye
  8. Spectrum Gold glaze (1112)
  9. Labels and safety for these seven glazes
  10. What these glazes do well
  11. Weak points
  12. Who should buy and who should skip
  13. Alternatives
  14. Frequently asked questions

Verdict

Spectrum Bougainvillea glaze (code 1447) is a cone 4/6 floating glaze from Spectrum's 1430 line: a pink base that breaks into violet, purple and coral where it pools, all from one jar. It is a good buy if you fire a cone 5 or 6 electric kiln, brush two to three coats and accept that the result shifts with thickness and clay body. Kimchi, Sangria, Shallot, Sunrise and Tiger Eye are its warm siblings in the same line. Spectrum Gold (1112) belongs to a different group, Stoneware Metallics, and carries a caution label.

The weak spot is information. Spectrum's own product pages show a name, sizes and a label icon and nothing more, so the color descriptions on this page come from dealer listings, and we say which dealer each time. This page is research-based: we compared Spectrum's product pages, its 2026 USD price list, color charts and safety data sheet with US and UK dealer listings in November 2026. We did not fire these glazes ourselves.

The seven warm Spectrum glazes at a glance

GlazeLineCone (Spectrum)FinishCoatsFood label as Spectrum states itLight vs dark clay note
1447 Bougainvillea1430 Floating (2024 colors)4/6 on site; 5/6 on price listGloss, reactive2 to 3 brushedAP icon; line text "lead-free and dinnerware safe"None published; chips on white clay
1436 Kimchi1430 Floating (first 12)4/6 on site; 5/6 on price listGloss, reactive2 to 3 brushedAP icon; same line textNone published
1435 Sangria1430 Floating (first 12)4/6 on site and chart; 5/6 on price listGloss, reactive2 to 3 brushedAP icon; same line textNone published
1448 Shallot1430 Floating (2024 colors)4/6 on site; 5/6 on price listGloss, reactive2 to 3 brushedAP icon; same line textNone published
1446 Sunrise1430 Floating (2024 colors)4/6 on site; 5/6 on price listGloss, reactive2 to 3 brushedAP icon; same line textNone published
1444 Tiger Eye1430 Floating (2024 colors)4/6 on site; 5/6 on price listGloss, reactive2 to 3 brushedAP icon; same line textNone published
1112 GoldStoneware Metallics (also listed in 1100)4/6 on site; chart says cone 5MetallicNot published for 1112CL label; left off the 1100 chart's non-toxic list; no dinnerware wording foundNone published

Spectrum's sources do not agree on every detail. Its site files the floating line under "Cone 4/6", the 2026 price list heads the section "Cone 5/6", and dealer copies of Spectrum's line text say the samples were fired at cone 5. Dealers repeat Spectrum's "2 to 3 coats for full coverage", while Sounding Stone's directions for the 2024 colors say three coats over cone 04 bisque, then fire to cone 5. Some dealers spell Tiger Eye as "Tiger's Eye"; Spectrum's own page and price list say Tiger Eye.

How the warm floating glazes behave

Spectrum named the line for its look: one color seems to float over another, without you layering two glazes. Dealer copies of the line text say the result depends on firing temperature, glaze thickness and the clay body, that the glazes break over texture, and that they can run on vertical surfaces. Fire to cone 5, about 2,167°F (1,186°C), or cone 6, about 2,232°F (1,222°C), on Orton's chart; our pottery cone chart lists both.

The line as a whole, with its 36 colors, sample packs, dipping and firing notes, has its own page: Spectrum floating glazes. This page sticks to the warm colors and the gold.

Spectrum Bougainvillea glaze (1447)

Bougainvillea 1447Spectrum 1447 Bougainvillea Floating Glaze, Cone 4/6
Key specs 1430 Floating; cone 4/6 (site), 5/6 (price list); 4 oz, pint, gallon, 10 lb dry
Mid-range tierCheck price on Amazon

Bougainvillea is one of the twelve 2024 floating colors (codes 1443 to 1454). Spectrum sells it as a 4 oz jar, pint, gallon and 10 lb dry bag, in the higher of the line's two price groups. Spectrum also picked it for its own six-pint floating econo pack, next to Pearl White, Kimchi, Scandinavian Blue, Fuzzy Peach and Spanish Moss, and it comes in the 12-jar sample set of the 2024 colors.

  • Code and line: 1447, 1430 Floating, cone 4/6
  • Look (Hot Clay listing): soft pink with "vibrant flows of violet, purple and coral pink"
  • Coats: 2 to 3 brushed, per dealer copies of Spectrum's line text
  • Sizes: 4 oz, pint, gallon, 10 lb dry
  • Label: AP icon on Spectrum's product page

Light vs dark clay: Spectrum publishes no dark-clay chip for Bougainvillea. Its chips are fired on white clay, so a buff, brown or speckled body will look different. Fire a test tile on the clay you use before you glaze a set of mugs.

Application: brush two to three even coats on bisque and let each coat dry before the next. Keep the lowest inch of the pot thinner, because floating glazes move. For a dipping bucket, Spectrum sells the 10 lb dry bag; it does not publish water ratios online, so ask your dealer for the mixing directions.

Bougainvillea glaze combinations

Spectrum publishes no layering combinations for Bougainvillea or any other floating color. What you find online are user results, mostly on Glazeshare, which are not maker-tested. The pairings shown on its Bougainvillea page include a Blue Rutile (AMACO makes the best known one, see our AMACO Blue Rutile guide), Chun Plum listed as PC-55, and Spectrum's own Shallot, Sunrise, Pearl White and Louisiana Bayou. Treat them as ideas for test tiles, not recipes. Our glaze combinations guide explains how to test pairs safely.

Pros

  • Pink with violet and coral breaks from one jar
  • Sold in a 4 oz jar for testing
  • In Spectrum's own econo pack

Cons

  • No maker description
  • Can run when thick
  • Higher price group

Who should skip it: potters who want a flat, even pink, and anyone firing low fire or cone 10.

Spectrum Kimchi glaze (1436)

Kimchi 1436Spectrum 1436 Kimchi Floating Glaze, Cone 4/6
Key specs 1430 Floating; cone 4/6 (site), 5/6 (price list); 4 oz, pint, gallon, 10 lb dry
Mid-range tierCheck price on Amazon

Kimchi is one of the first twelve floating colors (1431 to 1442), the group covered by Spectrum's floating safety data sheet dated January 2019. It sits in the higher price group and appears in both the 12-jar sample set of the first colors and Spectrum's six-pint econo pack. BuyMayco tags it orange; Hot Clay describes "a rich rust stoneware glaze with flowing tones of burnt orange and icy blue."

  • Code and line: 1436, 1430 Floating, cone 4/6
  • Look (Hot Clay listing): rust with burnt orange and icy blue
  • Coats: 2 to 3 brushed
  • Sizes: 4 oz, pint, gallon, 10 lb dry
  • Label: AP icon; dealers repeat "lead-free and dinnerware safe"

Light vs dark clay: not published by the maker. Spectrum's chips are on white clay, so test on your own body before a full set.

Application: buyer reviews on Hot Clay and Bath Potters for the line report a more mottled surface at two coats and fuller color at three. Spectrum has no separate coat count for Kimchi. If you want orange without the blue, look at Papaya (1445) or Curry (1432) on test tiles first; Spectrum does not describe either in words.

Pros

  • Warm rust and orange with a cool blue break
  • Two pack options include it
  • 4 oz size

Cons

  • Blue streaks may not suit every form
  • No maker coat count or description

Who should skip it: anyone after a solid orange, and potters without a cone 5 or 6 kiln.

Spectrum Sangria glaze (1435)

Sangria 1435Spectrum 1435 Sangria Floating Glaze, Cone 4/6
Key specs 1430 Floating; cone 4/6 (site and chart), 5/6 (price list); 4 oz, pint, gallon, 10 lb dry
Mid-range tierCheck price on Amazon

Sangria glaze is made by Spectrum Glazes Inc. of Concord, Ontario, Canada, as code 1435 in the 1430 Floating line. It is the one color named on the cover of Spectrum's floating color chart, which reads "New Floating Glazes, For Stoneware, fires Cone 4/6." Hot Clay describes it as "a rich raspberry stoneware glaze with a purple froth."

  • Code and line: 1435, 1430 Floating (first 12), cone 4/6
  • Look (Hot Clay listing): raspberry with a purple froth
  • Coats: 2 to 3 brushed
  • Sizes: 4 oz, pint, gallon, 10 lb dry
  • Label: AP icon on Spectrum's page

Light vs dark clay: not published by Spectrum. Bath Potters buyers report a pinky red over cherry red at about 2,192°F (1,200°C), and a pink, orange and red mix on a light stoneware. Glazeshare also has user tiles on brown speckled clay. Those are buyer results, so use them as a guide only.

Application: one Bath Potters buyer found two coats enough on textured surfaces and brushed extra on the top third to half for drips. That matches Spectrum's general advice that thickness drives the effect. Leave the foot area thin and fire on a kiln-washed shelf or a cookie.

Pros

  • Deep red and purple from one jar
  • Strong break on texture
  • Widely stocked

Cons

  • Higher price group
  • Color swings between cone 5 and cone 6

Who should skip it: potters who need a true, even red. A floating glaze will not give you that.

Shallot, Sunrise and Tiger Eye

These three are smaller sellers from the 2024 floating colors. All three share Bougainvillea's facts: cone 4/6, two to three brushed coats, the higher price group, an AP icon on Spectrum's page, and 4 oz, pint, gallon and 10 lb sizes. Spectrum describes none of them in words.

Spectrum Shallot glaze (1448)

Shallot 1448Spectrum 1448 Shallot Floating Glaze, Cone 4/6
Key specs 1430 Floating; cone 4/6 (site), 5/6 (price list); 4 oz, pint, gallon, 10 lb dry
Mid-range tierCheck price on Amazon

Hot Clay calls Shallot "a soft plum red stoneware glaze with flowing tones of lavender." It sits next to Bougainvillea on Spectrum's own related-products list, and Glazeshare users pair the two. Choose it over Sangria if you want a softer plum than raspberry. Skip it if you want a strong red or a fully opaque purple.

Spectrum Sunrise glaze (1446)

Sunrise 1446Spectrum 1446 Sunrise Floating Glaze, Cone 4/6
Key specs 1430 Floating; cone 4/6 (site), 5/6 (price list); 4 oz, pint, gallon, 10 lb dry
Mid-range tierCheck price on Amazon

Spectrum gives Sunrise no description; Creative Crafts tags it peach and pink, and The Ceramic Shop lists it as a cone 4/6 stoneware glaze, lead free, non-toxic and dinnerware safe. Do not confuse it with 1483 Sunset, a newer floating color on Spectrum's site that is not on the April 2026 price list. Skip it if you need to know exactly what you are getting before a test tile, because there is no maker chip description to go on.

Spectrum Tiger Eye glaze (1444)

Tiger Eye 1444Spectrum 1444 Tiger Eye Floating Glaze, Cone 4/6
Key specs 1430 Floating; cone 4/6 (site), 5/6 (price list); 4 oz, pint, gallon, 10 lb dry
Mid-range tierCheck price on Amazon

Spectrum lists it as 1444 Tiger Eye; Clay-King and Hot Clay write "Tiger's Eye". Hot Clay describes "a honey stoneware glaze with flows of golden yellow and purple." Krueger Pottery lists it by the pint and the gallon. It suits brown-toned ware where you want a honey color with a purple break. Skip it if purple in a honey glaze bothers you, or if you want a clear amber over carving.

Spectrum Gold glaze (1112)

Gold 1112Spectrum 1112 Gold Stoneware Metallic Glaze, Cone 4/6
Key specs Stoneware Metallics and 1100 series

Spectrum Gold is not a floating glaze. Spectrum files 1112 Gold under Stoneware Metallics with 1114 Gold Rain, 1116 Mirror and 1188 Pewter, and also lists it in its 1100 cone 4/6 series. It is a gold-colored metallic glaze, not a real gold luster; our gold glaze guide explains that difference and covers lusters.

  • Code and line: 1112, Stoneware Metallics and 1100 series, cone 4/6 (the 1100 chart says cone 5)
  • Finish: metallic gold (dealers list it as "Metallic Gold")
  • Coats: not published for 1112; Spectrum's 1100 chips were shot at three brush coats at cone 5 on white clay, per dealer copies
  • Sizes: pint, gallon, 10 lb dry (no 4 oz on Spectrum's page)
  • Label: CL icon on Spectrum's page; marked * (CL) on the 2026 price list; excluded from "NON TOXIC" on the 1100 chart

Light vs dark clay: not published by the maker. Food use: we found no dinnerware wording for 1112 from Spectrum or its dealers, so keep it to outside surfaces and decorative pieces. Mirror, its silver-toned sibling, is covered on our floating glazes page.

Pros

  • One-fire gold color at cone 4/6
  • Lower price group than the warm floating colors
  • Pint size

Cons

  • CL caution label
  • No dinnerware wording
  • No description or coat count from Spectrum

Who should skip it: anyone glazing the inside of mugs or bowls, and anyone who wants the bright shine of real gold luster.

Labels and safety for these seven glazes

Spectrum marks each product page with an ACMI seal. The six floating colors here show the AP (non-toxic) icon; Gold shows CL (caution label). Krueger Pottery's copy of Spectrum's text says CL glazes are not suitable for young children or pregnant women in the liquid state. For dinnerware, dealers repeat Spectrum's line text that the cone 4/6 floating glazes are lead-free and dinnerware safe, and Spectrum's 1100 chart adds that glazes must be fired to the recommended temperature to be dinnerware safe.

A label is the maker's result, not a promise about your pot. Runny, crazed or under-fired surfaces behave differently, and you cannot tell from looking. Our Spectrum glazes review explains the brand's full set of label icons.

Read Spectrum's safety data sheet (on its Health and Safety page) before you mix a 10 lb dry bag. Dry glaze contains silica: wear a NIOSH-approved respirator while mixing, wipe up with a damp sponge and never dry sweep. Protect kiln shelves with kiln wash or a cookie under runny glazes, and keep the kiln clearance and ventilation your kiln maker sets. Do not use the CL-labeled Gold on food surfaces.

What these glazes do well

  • Two-tone color from a single jar, with no layering needed.
  • 4 oz jars for the floating colors, so testing is cheap.
  • Pint, gallon and 10 lb dry sizes for brushing or dipping.
  • AP icons on all six floating colors here.

Weak points

  • No maker descriptions, coat counts or dark-clay notes on Spectrum's pages.
  • Cone labels differ between site, chart and price list.
  • Results move a lot with thickness and with cone 5 versus cone 6.
  • Gold has a caution label and no dinnerware wording.

Who should buy and who should skip

Buy these if you fire a cone 5 or 6 electric kiln, like surfaces that change across a pot, and will make test tiles first. Bougainvillea, Shallot and Sangria suit potters who want pinks, plums and reds; Kimchi and Tiger Eye suit rust and honey palettes; Sunrise sits in between.

Skip them if you want predictable, flat color, fire low fire or cone 10, or need clear written guidance from the maker. Skip Gold for anything that touches food.

Alternatives

  • AMACO red and purple glazes: Potter's Choice reds and purples with AMACO's own layering library.
  • Mayco red, pink and purple glazes: Mayco Stoneware colors with clearer maker labels.
  • Spectrum floating glazes: the cooler floating colors, Pearl White and Cactus, plus Spectrum Mirror and Moonscape.
  • Cone 6 glazes: our picks across brands for mid-fire kilns.

Sources: spectrumglazes.com 1430 Series Floating Glazes category (pages 1 and 2), product pages for 1435 Sangria, 1436 Kimchi, 1444 Tiger Eye, 1446 Sunrise, 1447 Bougainvillea, 1448 Shallot, 1112 Gold and ECONO1430.4 Econo Packs, Stoneware Metallics and 1100 Series categories; Spectrum 2026 High Fire USD price list; Spectrum 1100 and 1430 color charts; Spectrum Floating Stoneware Glazes SDS (rev. 2019, dealer-hosted); dealer listings from Krueger Pottery, The Ceramic Shop, Clay-King, Sounding Stone, BuyMayco, Creative Crafts, Clayworks Supplies, Hot Clay and Bath Potters; Glazeshare user combinations (user-submitted); Orton cone chart. Research-based: we compare maker pages and published data and did not fire these glazes. Specs checked November 2026.

Frequently asked questions

Who makes Sangria glaze?

The Sangria glaze potters usually mean is Spectrum 1435 Sangria, made by Spectrum Glazes Inc. in Concord, Ontario, Canada. It is a cone 4/6 floating glaze in the 1430 line, sold in the US through dealers such as The Ceramic Shop, Clay-King and Krueger Pottery.

What color is Spectrum Bougainvillea glaze?

It is a pink floating glaze that breaks into violet, purple and coral pink, according to dealer listings such as Hot Clay. Spectrum itself publishes only a color chip, so fire a test tile on your own clay to see your result.

What glazes go well with Spectrum Bougainvillea?

Spectrum publishes no combinations for it. User galleries such as Glazeshare show it with a Blue Rutile, Chun Plum and Spectrum Shallot, Sunrise, Pearl White and Louisiana Bayou. Those are user results, so test any pair on tiles with a catch dish first.

How many coats of Spectrum Kimchi should you use?

Dealer copies of Spectrum's line text say 2 to 3 coats for full coverage. Two coats tend to look thinner and more mottled, three give more color and more movement. Keep the bottom inch thinner because floating glazes can run.

Is Spectrum 1112 Gold glaze food safe?

We found no dinnerware wording for 1112 Gold from Spectrum or its dealers. It carries a CL (caution label) icon and is excluded from the non-toxic list on Spectrum's 1100 chart, so keep it off food and drink surfaces.

What is the difference between Spectrum Sunrise and Spectrum Sunset?

They are two different floating glazes. 1446 Sunrise is one of the 2024 colors on Spectrum's April 2026 price list; 1483 Sunset is a newer color shown on Spectrum's site but not on that price list. Check the code on the jar before you buy.

Is Spectrum Tiger Eye the same glaze as Tiger's Eye?

Yes. Spectrum names code 1444 Tiger Eye on its site and price list, and some dealers, such as Clay-King and Hot Clay, write Tiger's Eye. Search by the code 1444 to be sure you get the floating glaze.

Researched and written by Muhammad Mustafa

Muhammad Mustafa researches and writes Home Pottery HQ from maker spec sheets, manuals, dealer listings and published studio guidance. He does not claim hands-on testing of products he has not used, and every page names its sources.

Specifications and availability change often. Check the product listing before you buy, and follow the manufacturer's manual for setup, weight limits and maintenance. We do not print prices because they change daily; the buttons take you to the live price. Read our affiliate disclosure.