Review

AMACO Smokey Merlot and Other AMACO Red, Pink and Purple Glazes

Verdict in brief

AMACO Smokey Merlot (PC-57) is a cone 5 to 6 Potter's Choice glaze that AMACO describes as a warm, dark purple with a soft lilac float. It anchors AMACO's red, pink and purple range, which also includes Chun Plum, Deep Firebrick and Fire & Ice (Potter's Choice), Lunar Pink and Floating Lavender (Phase), Rose Mist (Potter's Choice Flux) and Acai Matte (Shino). All eight go on cone 04 bisque and fire to cone 5 to 6.

On this page
  1. Verdict
  2. The eight glazes at a glance
  3. AMACO Smokey Merlot (PC-57)
  4. AMACO Chun Plum (PC-55)
  5. AMACO Deep Firebrick (PC-59)
  6. AMACO Fire & Ice (PC-72)
  7. AMACO Lunar Pink (PG-54)
  8. AMACO Floating Lavender (PG-55)
  9. Flux and Shino members
  10. Food safety and labels
  11. What this group does well
  12. Weak points
  13. Who should buy, and who should skip
  14. Alternatives
  15. Safety notes
  16. Frequently asked questions

Verdict

For one dark purple that layers well, AMACO Smokey Merlot is the safest pick here. It comes in pints, gallons and a dry dipping mix, AMACO publishes a long list of pairings for it, and the Potter's Choice line sheet says the line stays stable beyond cone 6. Chun Plum is the softer, translucent pink-red; Deep Firebrick is the opaque, speckled brick red; Fire & Ice is the copper red, and AMACO says it needs three unthinned coats.

The pinks and lavenders are newer and sold in pints only. Lunar Pink and Floating Lavender are Phase glazes, which AMACO says are opaque even at one coat. Rose Mist is a Potter's Choice Flux glaze that moves more at cone 6. Acai Matte, a Shino, actually fires to blue and brown by AMACO's own description, and it showed as out of stock on AMACO's shop in November 2026.

This page is research-based: we compared AMACO's product pages, line sheet, blog posts and layering library. We have not fired these glazes ourselves.

The eight glazes at a glance

Entries come from AMACO's product pages unless a cell names another AMACO source. "Food label" is the seal shown on the product page in November 2026.

GlazeLineConeFinish and look (AMACO)Coats (AMACO)Food labelClay note
PC-57 Smokey MerlotPotter's Choice5 to 6Opaque; warm dark purple, lilac floatNot on product page; line sheet says heavy-handedNo Food Safe seal on page; line sheet says food safety statusNot published
PC-55 Chun PlumPotter's Choice5 to 6Translucent pink-red, light tan breakNot publishedFood Safe seal, APNot published
PC-59 Deep FirebrickPotter's Choice5 to 6Opaque, speckled brick redBlog example: 2 to 3 coats as a baseNo Food Safe seal on page; line sheet says food safety statusBlog: shows up well on a variety of clay bodies
PC-72 Fire & IcePotter's Choice5 to 6Opaque; deep red thick, icy blue thin3 brush coats, unthinnedCL seal, no Food Safe seal on pageNot published
PG-54 Lunar PinkPhase5 to 6Opaque pale cool pink3 to 4; 2 over 2 for layeringFood Safe seal, APNot published
PG-55 Floating LavenderPhase5 to 6Opaque light purple, lighter spots3 to 4; 2 over 2 for layeringFood Safe seal, APNot published
PCF-36 Rose MistPotter's Choice Flux5 to 6Blush pink, lavender hints, white swirls3 even coatsFood Safe seal, AP"Beautiful on any color of clay"
SH-22 Acai MatteShino5 to 6 (line)Matte; blue and brown shadesNot publishedFood Safe seal, APNot published

AMACO's shop listed pints at roughly $22 to $27 in November 2026, with gallons where offered costing more. Check the live price at your dealer.

AMACO Smokey Merlot (PC-57)

Dark purple, layers both waysAMACO Potter's Choice PC-57 Smokey Merlot Glaze
Key specs Cone 5 to 6; opaque dark purple with lilac float; pint, gallon, dry dipping mix
Mid-range tierCheck price on Amazon

AMACO calls Smokey Merlot "a warm, dark purple glaze with a soft float of lilac over the surface" and says it suits smooth surfaces, textured surfaces and layering with other Potter's Choice glazes. Its fall layering post adds that Smokey Merlot "can look different depending on what it's paired with", reading as a dark ruby over Matcha Matte Shino.

  • Line: Potter's Choice, cone 5 to 6 on cone 04 bisque (line sheet)
  • Formats: pint, gallon and a dry-mix dipping glaze
  • Labels: AP seal on the product page; no Food Safe seal shown there
  • Coats: not on the product page; the line sheet says most Potter's Choice glazes "benefit from a heavy-handed application"

AMACO publishes no light vs dark clay note for PC-57, and its blog combinations were fired on No. 11 A-Mix White Stoneware, a light body. On red or brown clay, test first; our dark clay bodies guide explains why iron in the clay shifts glaze color.

Brush it on heavily. For the dry dipping mix, AMACO warns that dry dipping glazes "can be difficult to layer", so test before a full piece.

Smokey Merlot glaze combinations

AMACO publishes these pairings by name in its layering library, line sheet or blog; coat counts appear only where AMACO states them.

  • Smokey Merlot on top: over PC-12 Blue Midnight, PC-21 Arctic Blue, PC-30 Temmoku, PC-43 Toasted Sage, PC-55 Chun Plum, PC-62 Textured Amber Brown, PCF-19 Cirrus Flow, PCF-74 River Birch, C-1 Obsidian, C-5 Charcoal, C-32 Ochre, C-36 Iron and C-55 Poppy
  • Blackberry Harvest: Smokey Merlot over SH-46 Matcha Matte, 3 coats over 3 coats, cone 6
  • Smokey Merlot underneath: PC-02 Saturation Gold, PC-23 Indigo Float, PC-33 Iron Lustre, PC-38 Iron Yellow and PC-41 Vert Lustre over Smokey Merlot

Our AMACO glaze layering guide covers order, thickness and drip control.

Pros

  • Three formats including gallon
  • Huge set of AMACO-published pairings
  • Works as base or top coat

Cons

  • No coat count on the product page
  • No Food Safe seal on the page itself

Who should skip it: Potters who want a bright or pastel purple; look at Floating Lavender instead.

AMACO Chun Plum (PC-55)

Translucent pink-redAMACO Potter's Choice PC-55 Chun Plum Glaze
Key specs Cone 5 to 6; translucent pink-red, light tan break; pint, gallon, dry dipping mix
Mid-range tierCheck price on Amazon

AMACO describes Chun Plum as "a pink-red translucent glaze that breaks light tan over textures". It says the glaze "imitates the copper reds of Asia but with a reliable color response in oxidation firings", and suggests layering it over other Potter's Choice glazes "for a warmer tone and hints of pink and red".

  • Line: Potter's Choice, cone 5 to 6
  • Formats: pint, gallon and a dry-mix dipping glaze
  • Labels: AP and Food Safe seals on the product page
  • Coats: not published by AMACO; The Ceramic Shop recommends three thick coats and warns a thin coat looks splotchy

AMACO gives no light vs dark clay note. Because it is translucent, the clay and any base glaze show through, so the same pint can look quite different on a white and a buff body.

AMACO's layering library lists Chun Plum over PC-20 Blue Rutile, PC-22 Blue Stone, PC-29 Deep Olive Speckle, PC-38 Iron Yellow, PC-44 Sage, PC-67 River Rock, PCF-75 Moss Mist, C-3 Smoke and C-54 Snapdragon. It also shows PC-57 Smokey Merlot and PC-59 Deep Firebrick over Chun Plum.

Pros

  • Food Safe seal on the page
  • Copper-red look from an electric kiln
  • Good warm top coat

Cons

  • Translucent, so results depend on clay
  • No coat count from AMACO

Who should skip it: Anyone who wants a solid, opaque red that hides the clay.

AMACO Deep Firebrick (PC-59)

Opaque speckled redAMACO Potter's Choice PC-59 Deep Firebrick Glaze
Key specs Cone 5 to 6; opaque speckled brick red; pint, gallon, dry dipping mix
Mid-range tierCheck price on Amazon

AMACO's description: "an opaque, speckled brick red glaze that breaks translucent where thin". It says this "bold, dark red glaze" layers well under or over other Potter's Choice glazes. It also warns the glaze "contains black specks that may clog spray guns" and should be well mixed so the speckles spread evenly.

  • Line: Potter's Choice, cone 5 to 6
  • Formats: pint, gallon and a dry-mix dipping glaze
  • Labels: AP seal on the product page; no Food Safe seal shown there
  • Coats: not on the product page; AMACO's blog uses 2 to 3 coats as a base

AMACO's customer-favorites post says Deep Firebrick and Arctic Blue "show up well on a variety of clay bodies" at cone 5 or 6, the closest it comes to a clay note here.

Published pairings: 2 coats of PC-21 Arctic Blue as an accent over 2 to 3 coats of Deep Firebrick; "Maple Butter", with 2 coats of PCF-18 Honeydew on the top third over 2 coats of Deep Firebrick, cone 6; Deep Firebrick over PC-30 Temmoku, PC-43 Toasted Sage, PC-45 Dark Green, PC-55 Chun Plum and PC-56 Ancient Copper; and PC-23 Indigo Float over Deep Firebrick.

Pros

  • Opaque red that hides the clay
  • Wide cone 5 or 6 range per AMACO
  • Strong partner for blues

Cons

  • Specks can clog a spray gun
  • Must be stirred well

Who should skip it: Potters who spray glaze, or who want a clean red with no speckle.

AMACO Fire & Ice (PC-72)

Copper red for electric kilnsAMACO Potter's Choice PC-72 Fire & Ice Glaze, Pint
Key specs Cone 5 to 6; deep red thick, icy blue thin; 3 unthinned brush coats; pint
Mid-range tierCheck price on Amazon

AMACO says Fire & Ice "is deep red where thick and icy blue where thin", and calls it "a reduction copper red for electric firing" with a blue break on texture. It also gives the clearest instruction in this group: "Apply three coats for best oxblood red color", and "do not thin the glaze".

  • Line: Potter's Choice, cone 5 to 6 on cone 04 bisque
  • Formats: pint only on AMACO's shop
  • Labels: CL (cautionary label) seal on the product page, not AP; no Food Safe seal shown there
  • Coats: 3 brush coats, each dried before the next

AMACO publishes no clay note. It says Fire & Ice layers well over Celadons, Potter's Choice and Satin Matte glazes, and that layers "may run if paired with a runny glaze". Thickness sets the color: a thin coat gives the blue, not the red.

Pros

  • True oxblood look from an electric kiln
  • Clear coat instructions
  • Dramatic break on texture

Cons

  • CL seal, so read the SDS
  • Pint only
  • Thin spots go blue

Who should skip it: Dippers and anyone who brushes thin coats.

AMACO Lunar Pink (PG-54)

Pale pink Phase glazeAMACO Phase Glaze PG-54 Lunar Pink, Pint
Key specs Cone 5 to 6; pale cool pink; 3 to 4 brush coats, 2 over 2 for layering; pint
Mid-range tierCheck price on Amazon

AMACO describes Lunar Pink as a pale, cool pink that shows white visual texture where it is thick, and compares it to sunlight scattering through the atmosphere at moonrise. It belongs to the Phase line, which AMACO's Phase blog post describes as opaque glazes for cone 5 to 6 that "develop a subtle mottling where they're thick".

  • Line: Phase (PG), cone 5 to 6 on cone 04 bisque
  • Formats: pint only
  • Labels: AP and Food Safe seals on the product page
  • Coats: 3 to 4 brush coats, unthinned; 2 coats over 2 coats for layering

The Phase post says these glazes are "opaque, even at one coat", "stable when used alone", and "can flow dramatically" when layered, and warns that going too thick when layering may cause bubbling. AMACO gives no clay note.

AMACO says Lunar Pink layers well over Celadons, Potter's Choice and Satin Matte glazes. Its product photos show it over SM-11 White and over PC-17 Honey Flux at cone 6.

Pros

  • Opaque at one coat per AMACO
  • Food Safe seal
  • Clear coat counts

Cons

  • Pint only
  • Can bubble when layered too thick

Who should skip it: Potters after a strong pink or a red.

AMACO Floating Lavender (PG-55)

Light purple Phase glazeAMACO Phase Glaze PG-55 Floating Lavender, Pint
Key specs Cone 5 to 6; light purple with lighter spots; 3 to 4 brush coats; pint
Mid-range tierCheck price on Amazon

AMACO calls Floating Lavender "a light purple with lighter visual spot texture where thick" that is "light and airy as a cloud at sunset". Application matches Lunar Pink: 3 to 4 unthinned brush coats on cone 04 bisque, or 2 coats over 2 coats for layering.

  • Line: Phase (PG), cone 5 to 6
  • Formats: pint only
  • Labels: AP and Food Safe seals on the product page
  • Clay note: not published by AMACO

AMACO's Phase post shows it as 2 coats over 3 coats of SM-11 White Satin Matte at cone 6, over C-1 Obsidian at 2 coats each, and mixed in equal parts with PG-42 Teal Drift. Product photos add Floating Lavender over PC-17 Honey Flux.

Naming conflict: AMACO's product page says PG-55, but one Phase blog caption says PG-56, and some dealers spell it "Floating Lavendar". Order by PG-55.

Pros

  • Soft purple that stays opaque
  • Food Safe seal
  • Mixes with Teal Drift per AMACO

Cons

  • Pint only
  • Code and spelling vary at dealers

Who should skip it: Anyone who wants the dark purple of Smokey Merlot.

Flux and Shino members

These two belong to lines with their own pages here, so they get short entries.

AMACO Rose Mist (PCF-36)

Blush pink flux glazeAMACO Potter's Choice Flux PCF-36 Rose Mist Glaze, Pint
Key specs Cone 5 to 6 (more fluid at 6); blush pink with lavender and white; 3 coats; pint
Mid-range tierCheck price on Amazon

AMACO: "a soft, blush-pink base, with subtle hints of lavender and white swirls", good as a base or top coat and "Beautiful on any color of clay". It is "Good at cone 5, more fluid at cone 6", goes on in 3 even coats over cone 04 bisque, and carries AP and Food Safe seals. Product photos show PC-57 Smokey Merlot and PC-21 Arctic Blue over Rose Mist. Pint only. The flux line as a whole is covered in our AMACO flux glazes guide.

Who should skip it: Cone 6 potters who cannot risk any extra flow.

AMACO Acai Matte (SH-22)

Matte Shino, blue and brownAMACO Shino SH-22 Acai Matte Glaze, Pint
Key specs Cone 5 to 6 (Shino line); matte; blue and brown shades; pint
Mid-range tierCheck price on Amazon

Despite the berry name, AMACO describes Acai Matte as "a matte, 100% mixable mid-fire glaze that yields wonderfully varied shades of blue and brown", with color that varies with thickness. The page shows AP and Food Safe seals and no coat count. AMACO's shop showed it out of stock in November 2026 without calling it discontinued; SH-21 Acai Gloss is the glossy partner. AMACO's library lists PC-24 Sapphire Float over Acai Matte. See our AMACO Shino glazes page for the line.

Who should skip it: Anyone who wants a purple result.

Food safety and labels

AMACO's Potter's Choice line sheet says: "All Potter's Choice glazes hold a food safety status except PC-4 Palladium, PC-9 Vintage Gold and PC-64 Aventurine." None of the four here is an exception, yet the Smokey Merlot, Deep Firebrick and Fire & Ice pages did not show the Food Safe seal in November 2026, while Chun Plum did. The Phase, Flux and Shino glazes all showed it.

Fire & Ice carries AMACO's CL seal instead of AP. A CL product contains materials that need a caution label, so read its SDS before use. The AP or CL seal is about handling, not food use.

A Food Safe seal describes one glaze, fired to the stated cone, on its own. A layered pair is a new glaze no one has tested on your clay, and runny or underfired surfaces are not ones to trust. We cannot promise any of these glazes is food safe on your pots. Keep untested combinations off the inside of mugs and bowls, and read our food safe glaze guide on testing.

What this group does well

  • Pale pink to near-black purple, all at cone 5 to 6.
  • Smokey Merlot, Chun Plum and Deep Firebrick come in gallons and dry mixes.
  • A large set of AMACO-named pairings to start from.
  • Phase glazes give clear coat counts and opaque color at one coat.

Weak points

  • No AMACO coat count for four of the eight.
  • Food Safe seals differ between the line sheet and three product pages.
  • Fire & Ice, the Phase glazes and Rose Mist are pint only.
  • Acai Matte was out of stock at AMACO and is not really purple.
  • Little clay guidance; you need test tiles.

Who should buy, and who should skip

Buy Smokey Merlot or Deep Firebrick for a dependable dark layering base, Chun Plum for a warm translucent top coat, and Fire & Ice for an oxblood red if you will brush three full coats. Lunar Pink and Floating Lavender suit potters who want soft, opaque pastels.

Skip this family if your kiln only reaches cone 05; none of these is made for low fire. Skip Rose Mist and layered Fire & Ice if you fire hot cone 6 with no cookies or kiln wash under the pots.

Alternatives

Our Potter's Choice glazes review covers the line. AMACO's blues, which pair with Smokey Merlot and Deep Firebrick, are on our AMACO Indigo Float and blue glazes page. For warmer browns and coppers, see AMACO earth tone glazes. If you use Mayco, the closest family is in our Mayco red, pink and purple glazes guide.

Safety notes

  • Dry dipping mixes contain silica: mix them wearing a NIOSH-approved respirator and wet clean; never dry sweep.
  • Read AMACO's SDS for every glaze, especially the CL-labeled Fire & Ice.
  • Wax the foot, leave a bare band, and fire layered pots on a cookie or a coated shelf.
  • Keep your kiln maker's clearance and ventilation figures; kilns run hot outside.

Sources: AMACO product pages for PC-57 Smokey Merlot, PC-55 Chun Plum, PC-59 Deep Firebrick, PC-72 Fire & Ice, PG-54 Lunar Pink, PG-55 Floating Lavender, PCF-36 Rose Mist and SH-22 Acai Matte (shop.amaco.com); AMACO Potter's Choice line sheet (amaco.com); AMACO blog posts "Exploring Phase Glazes", "AMACO Fall Layering Favorites" and "Customer Favorite AMACO Glaze Combinations to Try"; AMACO layering library entry titles (amaco.com/resources/layering); The Ceramic Shop listing for PC-55. Research-based: we compare maker pages and published data and did not fire these glazes. Specs checked November 2026.

Frequently asked questions

What color is AMACO Smokey Merlot?

AMACO describes Smokey Merlot (PC-57) as a warm, dark purple with a soft float of lilac over the surface. Over Matcha Matte Shino, AMACO says it reads as a dark ruby, so the base glaze and clay change what you see.

Is Smokey Merlot a stable glaze?

AMACO prints no run warning on the PC-57 page, and its Potter’s Choice line sheet says the line remains stable beyond cone 6. Layered under or over a fluid glaze it can still move, so wax the foot and fire layered pieces on a cookie until you have tested them.

Which AMACO red and purple glazes are least likely to run?

AMACO calls its Phase glazes (Lunar Pink, Floating Lavender) stable when used alone, and says the Potter’s Choice line stays stable beyond cone 6. Rose Mist is the one to watch, since AMACO says it is more fluid at cone 6, and any glaze here can run when layered with a runny glaze.

Is AMACO Fire and Ice a real copper red?

AMACO calls PC-72 Fire & Ice a reduction copper red for electric firing, deep red where thick and icy blue where thin. It recommends three unthinned brush coats on cone 04 bisque for the best oxblood color.

What is the difference between Chun Plum and Smokey Merlot?

Chun Plum is a translucent pink-red that breaks light tan over texture, so clay and base glaze show through. Smokey Merlot is an opaque, dark purple with a lilac float. AMACO publishes Smokey Merlot over Chun Plum as a combination.

What are AMACO Phase glazes?

Phase (PG) glazes are AMACO’s opaque cone 5 to 6 glazes that mottle where thick. AMACO says they are stable alone, can flow when layered, and are food safe and lead free; it recommends 3 to 4 brush coats, or 2 over 2 for layering.

What color is AMACO Acai Matte?

Not purple. AMACO describes SH-22 Acai Matte as a matte Shino that gives varied shades of blue and brown depending on thickness. It showed as out of stock on AMACO’s shop in November 2026.

Researched and written by Muhammad Mustafa

Muhammad Mustafa researches and writes Home Pottery HQ from maker spec sheets, manuals, dealer listings and published studio guidance. He does not claim hands-on testing of products he has not used, and every page names its sources.

Specifications and availability change often. Check the product listing before you buy, and follow the manufacturer's manual for setup, weight limits and maintenance. We do not print prices because they change daily; the buttons take you to the live price. Read our affiliate disclosure.