Verdict
A Spectrum floating glaze is worth buying if you fire a cone 5 or 6 electric kiln and want a layered, two-tone surface without layering two glazes. The 1430 line now lists 36 colors on Spectrum's site, sold in 4 oz jars, pints, gallons and 10 lb dry bags, with two 12-jar sample packs at dealers. The trade-off is guidance: Spectrum's pages give names, sizes and a label icon only, so you rely on dealer copies of its line text and on your own test tiles.
This page covers the line itself, then the cool and neutral glazes people search for with it: Pearl White and Cactus from the floating line, and Mirror and Moonscape, which are not floating glazes at all. The warm floating colors (Bougainvillea, Kimchi, Sangria and others) are on our Spectrum warm glaze colors page. Research-based: we compared Spectrum's site, 2026 price list, charts and SDS with US and UK dealer listings in November 2026, and did not fire these glazes.
What a Spectrum floating glaze is
Spectrum's own line text, as printed by Alabama Art and Blick, says the name came from the idea that the colors "should give the appearance of one color floating on top of another color." It calls them glossy, reactive mid-fire glazes with multi-tone, multi-color effects, "compatible with many other Spectrum stoneware glazes," and recommends firing at cone 5/6. Krueger Pottery's copy of the same text adds that "floating" is not a technical term, just a name for the look.
In practice, a floating glaze separates as it melts. The top color gathers on edges and high points or flows into a second color where the glaze is thick. That is why thickness, texture and the clay body change the result so much.
The four glazes on this page at a glance
| Glaze | Line | Cone (Spectrum) | Finish | Coats | Food label as Spectrum states it | Light vs dark clay note |
|---|---|---|---|---|---|---|
| 1431 Pearl White | 1430 Floating (first 12) | 4/6 on site; 5/6 on price list | Gloss, reactive | 2 to 3 brushed | AP icon; line text: lead-free, non-toxic, food safe | None published |
| 1438 Cactus | 1430 Floating (first 12) | 4/6 on site; 5/6 on price list | Gloss, reactive | 2 to 3 brushed | AP icon; same line text | None published |
| 1116 Mirror | Stoneware Metallics (also listed in 1100) | 4/6 on site; chart says cone 5 | Metallic | Not published for 1116 | CL label; left off the 1100 chart's non-toxic list; no dinnerware wording found | None published |
| 1115 Moonscape | 1100 series | 4/6 on site; chart says cone 5 | Gloss, reactive | 3 brushed on the sample (dealer) | AP icon; The Ceramic Shop: lead free, dinnerware safe | Brighter on white clay than dark (The Ceramic Shop) |
Every color in the 1430 Floating line
Spectrum's site lists 36 floating colors in three groups. The first twelve are covered by Spectrum's floating SDS dated 2019, the next twelve are what Sounding Stone sells as the "2024 Floating Glazes", and twelve newer codes from 1481 show on Spectrum's site but not on its April 2026 USD price list. The price list sorts the older 24 into a lower and a higher price group.
| Codes | Colors | Price group (2026 list) | Where we cover them |
|---|---|---|---|
| 1431, 1437, 1438, 1439, 1440, 1441, 1442 | Pearl White, Floating Celadon, Cactus, Nori Green, Floating Blue, Scandinavian Blue, Glacier | Lower | Pearl White and Cactus below |
| 1432, 1433 | Curry, Twilight | Lower | Table only |
| 1434, 1435, 1436 | Autumn Purple, Sangria, Kimchi | Higher | Sangria and Kimchi on the warm colors page |
| 1443 to 1448 | Fuzzy Peach, Tiger Eye, Papaya, Sunrise, Bougainvillea, Shallot | Higher | Tiger Eye, Sunrise, Bougainvillea and Shallot on the warm colors page |
| 1449 to 1454 | Floating Turquoise, Morning Glory, Louisiana Bayou, Spanish Moss, Ginger, Tapenade | Lower | Table only |
| 1481 to 1492 | Misty Pink, Rosewood, Sunset, Lemon Ginger, Purple Shimmer, Dusk Blue, Oyster Mushroom, Matcha, Seafoam, Smokey Heather, Misty Morning, Aegean Sea | Not on the April 2026 list | Table only |
Pints in the lower group typically run about $15 to $18 at US dealers in November 2026 and the higher group about $18 to $21; 4 oz jars are usually under $10. Check the live price, since dealers set their own.
How to apply Spectrum floating glazes
Brushing
Dealer copies of Spectrum's line text say 2 to 3 coats for full coverage, to test thickness for the look you want, and to thin with water if needed. Sounding Stone's directions for the 2024 colors are more exact: shake or stir well, brush three coats with a soft brush over bisque fired to cone 04, dry-foot or stilt the piece, then fire to cone 5.
- Stir the jar well; floating glazes settle.
- Brush the first coat in one direction and let it dry to the touch.
- Brush the second and third coats across the first, stopping about an inch above the foot.
- Add an extra coat on the rim or top third only if you want more flow.
- Wipe the foot clean and fire on a kiln-washed shelf or a cookie.
Dipping from a 10 lb dry bag
Spectrum sells every 1430 color as a 10 lb dry mix, which is the route to a dipping bucket. It does not publish water ratios or specific gravity for these glazes online, so ask your dealer for the mixing sheet and dip a test tile before a full piece. Mix dry glaze outdoors or under extraction while wearing a NIOSH-approved respirator.
Do Spectrum floating glazes run?
They can. Dealer copies of the line text warn that the glazes may run on vertical surfaces and tell you to protect kiln shelves; buyer reviews on Hot Clay say the same for Pearl White. Thin coats near the base, a clean foot and a coat of kiln wash on the shelf are the cheap insurance.
Firing: cone 5 versus cone 6
Spectrum's chips are shown at cone 5, and dealer text warns that changes in temperature change the look. Sounding Stone notes that cone 6 gives different variations than cone 5. On Orton's chart, cone 5 is about 2,167°F (1,186°C) and cone 6 about 2,232°F (1,222°C); our cone chart has the full table. If your kiln fires hot, start at cone 5 and fire a witness cone so you know what heatwork the tiles saw.
Spectrum floating glaze sample pack
Dealers sell two 12-jar sets of 4 oz jars, one for each of the two older groups:
- Sample pack 1 (1431 to 1442): Pearl White through Glacier. The Ceramic Shop lists it as "1430.1 Sample Pack 4oz".
- Sample pack 2 (1443 to 1454): Fuzzy Peach through Tapenade. Clay-King sells it as "Set #2", and Sounding Stone as the 2024 sample pack.
Twelve-jar packs typically cost about $55 to $100 at US dealers; check the live price. We found no sample pack for the 1481 to 1492 colors.
Spectrum also sells a six-pint econo pack on its own site (ECONO1430.4) with 1431 Pearl White, 1436 Kimchi, 1441 Scandinavian Blue, 1443 Fuzzy Peach, 1447 Bougainvillea and 1452 Spanish Moss.
Pack contents differ by seller. Spectrum's econo pack page and price list name the six colors above, while The Ceramic Shop's "1430.1" six-pint pack lists 1431 to 1436 instead. Read the codes on the listing before you order.
Spectrum floating glaze combinations
Spectrum publishes no floating-on-floating combinations. Its line text only says the floating glazes are compatible with many other Spectrum stoneware glazes. The combinations Spectrum does print are on its Nova and Ash chart, which pairs each Ash glaze with an 1100 series glaze; one of those pairs, 1425 Kiwi Ash with 1115 Moonscape, involves a glaze on this page. Our Spectrum glazes review lists all six Ash pairings.
Everything else you see online, from Glazeshare to Facebook groups, is user results. They are useful for ideas, but order of coats, thickness, clay and cone all differ. Test any pair on a tall, textured tile standing in a catch dish, and see our glaze combinations guide for a test routine that works across brands.
Spectrum Pearl White glaze (1431)
Pearl White is code 1431, the first color in the floating line, in the lower price group. It is in sample pack 1 and in Spectrum's own six-pint econo pack, which makes it one of the easiest floating colors to find. Hot Clay describes "a transparent pearl white stoneware glaze with flows of pale sand."
- Code and line: 1431, 1430 Floating, cone 4/6
- Look (Hot Clay listing): transparent pearl white with pale sand flows
- Coats: 2 to 3 brushed
- Sizes: 4 oz, pint, gallon, 10 lb dry
- Label: AP icon on Spectrum's page
Light vs dark clay: Spectrum publishes no note. Because dealers describe it as transparent, expect your clay color to show through it. Application: a Hot Clay buyer showed two coats over buff clay and warned that it runs, so keep it off the bottom inch. It is also a common top or bottom layer in user combinations.
Pros
- Lower price group
- Easy to find in packs
- A soft white that lets clay and texture show
Cons
- Runs when thick
- Not an opaque white
Who should skip it: potters who want a solid, liner-style white. A plain opaque white glaze will be more predictable.
Spectrum Cactus glaze (1438)
Cactus is code 1438, also in the first twelve floating colors and the lower price group. Hot Clay describes "a vibrant green stoneware glaze with flowing tones of lime green, moss, and soft olive", and the Czech dealer 1240.design adds a pearly sheen and 2 to 3 coats at about 2,192°F (1,200°C).
- Code and line: 1438, 1430 Floating, cone 4/6
- Look (dealer listings): bright green with lime, moss and olive
- Coats: 2 to 3 brushed
- Sizes: 4 oz, pint, gallon, 10 lb dry
- Label: AP icon on Spectrum's page
Light vs dark clay: not published by the maker; its chips are on white clay, so test on darker bodies. Do not confuse it with 1424 Cactus Ash, a separate Ash layering glaze Spectrum pairs with 1145. The floating SDS table prints "1468 Cactus", which looks like a typo for 1438.
Pros
- Lively green with several tones
- Lower price group
- In sample pack 1
Cons
- Easy to mix up with Cactus Ash
- No maker description
Who should skip it: anyone who wants a quiet celadon green. Floating Celadon (1437) or a semi-transparent glaze will be calmer.
Spectrum Mirror glaze (1116)
Mirror is not a floating glaze. Spectrum files 1116 Mirror under Stoneware Metallics with 1112 Gold, 1114 Gold Rain and 1188 Pewter, and also lists it in the 1100 series. Dealers sell it as "Metallic Mirror". Spectrum shows a CL icon on its page, marks it * (CL) on the 2026 price list, and leaves it off the non-toxic list on the 1100 chart.
- Code and line: 1116, Stoneware Metallics and 1100, cone 4/6 (chart says cone 5)
- Finish: metallic
- Coats: not published for 1116
- Sizes: pint, gallon, 10 lb dry
- Label: CL; no dinnerware wording found
Light vs dark clay: not published by Spectrum. Application: The Ceramic Shop lists it as a brushing glaze like the rest of the 1100 series. Keep it to outside surfaces. Its gold sibling, 1112 Gold, is on our warm colors page, and our metallic glaze guide compares metallic finishes across brands.
Pros
- Metallic look in one cone 4/6 firing
- Lower price than lusters
- Pint size
Cons
- CL caution label
- No dinnerware wording
- No maker description
Who should skip it: anyone glazing food surfaces, and potters with children helping in the studio.
Spectrum Moonscape glaze (1115)
Moonscape is code 1115 in Spectrum's 1100 cone 4/6 series, not the floating line. Spectrum's page shows an AP icon and sizes up to a 50 lb dry bag. Some dealers list it as "Textured Moonscape" or "Text. Moonscape", while Spectrum's site and 1100 chart just say Moonscape. The Ceramic Shop describes blues and greens that look more like the ocean than the moon, glossy with a textured surface.
- Code and line: 1115, 1100 series, cone 4/6 (chart says cone 5)
- Look (The Ceramic Shop): blue and green reactive gloss
- Coats: sample shown at three brushed coats on white clay (dealer)
- Sizes: pint, gallon, 10 lb, 50 lb dry
- Label: AP icon; The Ceramic Shop: lead free, non-toxic, dinnerware safe
Light vs dark clay: The Ceramic Shop says it looks brighter on white clays than on darker ones. Layering: Spectrum's Nova and Ash chart pairs it with 1425 Kiwi Ash, the one maker-published combination for any glaze on this page.
Pros
- Maker-published Ash pairing
- AP icon
- 50 lb dry size for dipping
Cons
- Name confusion between dealers
- Muted on dark clay
Who should skip it: potters who want a stable, even blue for tableware sets.
Food labels and safety
For the first twelve colors, Spectrum's line text says eleven are lead-free, non-toxic and food safe, and "the lone exception is 1439," Nori Green, which is above the non-toxic limit for copper. The 2019 floating SDS lists copper only for 1439. Pearl White and Cactus show AP icons on Spectrum's pages.
The newer colors need a closer look: the pages we checked for the 1481 to 1492 group (1481, 1482, 1486, 1489 and 1492) show an ACMI CL seal. Check each code's icon before you buy for mugs or bowls. Spectrum's 1100 chart adds that glazes must be fired to the recommended temperature to be dinnerware safe. A maker label is not a promise about your pot: runny, crazed or under-fired surfaces change things, so test finished ware if you sell it.
Read Spectrum's SDS before mixing dry glaze. Glaze dust contains silica: use a NIOSH-approved respirator for dry materials, clean with a damp sponge or mop, and never dry sweep. Our clay dust safety guide covers the studio routine. Keep kiln clearance and ventilation as your kiln maker states, and keep CL-labeled glazes such as Mirror off food surfaces.
What the floating line does well
- Two-tone, layered color from one jar.
- Four sizes, including 4 oz testers and 10 lb dry for dipping.
- Two 12-jar sample packs and a six-pint econo pack.
- AP icons on most of the older 24 colors.
Weak points
- No written descriptions, coat counts or firing notes on Spectrum's product pages.
- Cone wording differs between site (4/6), price list (5/6) and dealer text (samples at cone 5).
- Newest colors show CL seals on the pages we checked and are missing from the 2026 price list.
- Runs on vertical walls when applied thick.
Who should buy and who should skip
Buy Spectrum floating glazes if you fire to cone 5 or 6, like reactive surfaces, and will start with a sample pack and test tiles. Pearl White is the easy entry; Cactus suits bright greens. Moonscape suits potters who want a blue-green reactive glaze with a maker-published Ash pairing.
Skip them if you want flat, repeatable color across a dinner set, cannot protect your shelves from runs, or want detailed maker instructions. Skip Mirror for food surfaces.
Alternatives
- AMACO blue float glazes: Indigo Float and other AMACO floats with published layering.
- Mayco blue and green glazes: Mayco Stoneware blues and greens with clearer labels.
- Cone 6 firing schedule: how a slow cool changes reactive glazes like these.
Sources: spectrumglazes.com 1430 Series Floating Glazes category (pages 1 and 2), Mid Range, High Fire Cone 4/6, Stoneware Metallics and 1100 Series categories; product pages for 1431 Pearl White, 1438 Cactus, 1439 Nori Green, 1481 Misty Pink, 1482 Rosewood, 1486 Dusk Blue, 1489 Seafoam, 1492 Aegean Sea, 1115 Moonscape, 1116 Mirror and ECONO1430.4; Spectrum 2026 High Fire USD price list; Spectrum 1100, 1430 and 1500/1420 color charts; Spectrum Floating Stoneware Glazes SDS (rev. 2019, dealer-hosted); dealer listings from Alabama Art, Blick, Krueger Pottery, The Ceramic Shop, Clay-King, Sounding Stone, Potclays, Hot Clay, Bath Potters and 1240.design; Glazeshare user combinations (user-submitted); Orton cone chart. Research-based: we compare maker pages and published data and did not fire these glazes. Specs checked November 2026.