Pottery terms can make a first class or a clay catalog feel like a foreign language. Most of them simply name a material, a stage of drying, a way of shaping clay or a step in firing. This glossary groups the words you will meet as a US hobby potter by where they come up: clay, forming, drying, glazing and decorating, firing, kilns and tools. Each entry is a short definition only. Where we have a full guide to the term, the name links to it.
The definitions follow how US makers such as AMACO, Laguna, Orton, Skutt and Paragon use these words in their catalogs and manuals. Checked November 2026.
Clay terms
- Clay: fine-grained earth made mostly of clay minerals such as kaolinite that turns plastic when wet and permanently hard when fired. See what clay is made of.
- Clay body: a blend of clays and other minerals mixed to work and fire in a set way. Most clay you buy is a clay body. See types of pottery clay.
- Earthenware: low-fire clay, usually fired around cone 06 to 04, that stays porous unless glazed.
- Terracotta: red, iron-rich earthenware, used for planters and unglazed ware.
- Low fire clay: any clay body made to mature at low cones, mostly earthenware.
- Stoneware: dense mid-fire or high-fire clay, usually cone 5 to 10, fired cream, buff, gray or brown.
- Porcelain: fine white clay built on kaolin that fires dense and can be translucent when thin. Our stoneware vs porcelain page compares the two.
- Kaolin (china clay): a pure white primary clay, the base of porcelain and many glazes.
- Ball clay: a fine, very plastic clay added to bodies to make them easier to throw.
- Fire clay: a coarse clay that tolerates high heat, used in stoneware, sculpture bodies and kiln parts.
- Grog: crushed fired clay mixed into a body to add tooth, cut shrinkage and help thick work dry evenly.
- Speckled clay: a body with added iron or manganese specks that show through glaze.
- Dark clay: brown to black bodies colored with iron, manganese or stains.
- Paper clay: clay with paper fiber mixed in, lighter and stronger when dry, used for sculpture and joins.
- Raku clay: an open, grogged body made to survive the thermal shock of raku firing.
- Air-dry clay: a craft clay that hardens without a kiln; it is not ceramic and is not waterproof or food safe. See pottery without a kiln.
- Moist clay: ready-to-use clay sold wet in bags, usually 25 lb or 50 lb boxes.
- Dry clay (powdered clay): clay sold as powder that you mix with water yourself.
- Plasticity: how well wet clay bends and holds shape without cracking.
- Wedging: kneading clay by hand to even out moisture and push out air.
- Pugging: mixing and de-airing clay in a pug mill instead of by hand.
- Reclaim: recycling scraps and trimmings by drying, soaking (slaking) and rewedging them.
- Slip: clay thinned with water to a creamy liquid, used for joins, decoration and casting.
- Shrinkage: how much smaller clay gets as it dries and fires, given by makers as a percentage.
- Absorption: how much water fired clay soaks up, as a percentage; lower means denser. See stoneware clay.
- Maturing cone: the cone at which a clay body reaches its intended density and strength.
Forming terms
- Throwing: shaping clay on a spinning potter's wheel.
- Centering: pressing spinning clay until it runs true in the middle of the wheelhead.
- Opening: pressing down into centered clay to start the inside and set the floor.
- Pulling: squeezing the clay wall upward to make it taller and thinner.
- Compressing: pressing the floor or rim with a rib or sponge to firm the clay and prevent cracks.
- Throwing off the hump: making several small pieces from one large mound of centered clay.
- Bat: a removable disk fixed to the wheelhead so you can lift a pot off without touching it.
- Kick wheel: a potter's wheel powered by pushing a heavy flywheel with your foot.
- Banding wheel: a hand-turned turntable for decorating and hand-building.
- Splash pan: the tray around the wheelhead that catches water and slurry.
- Trimming: shaving a leather-hard pot upside down on the wheel to refine the base and cut a foot.
- Foot ring: the raised ring on the base of a pot, usually cut when trimming.
- Hand building: forming clay without the wheel, by pinching, coiling or slabs.
- Pinch pot: a pot shaped by pressing a ball of clay between thumb and fingers.
- Coiling: building walls from rolled ropes of clay joined together.
- Slab building: making forms from flat sheets of rolled clay.
- Slab roller: a machine that presses clay into even flat slabs.
- Extruder: a tool that pushes clay through a shaped die to make coils, tubes or handles.
- Score and slip: roughening two surfaces and adding slip so they bond.
- Pulling a handle: stretching a strap of wet clay by hand to make a mug handle.
- Sprigging: pressing small molded clay shapes onto a pot as decoration.
- Mold: a form, often plaster, that clay is pressed into or over (press, hump and slump molds).
- Slip casting: pouring liquid casting slip into a plaster mold to make hollow pieces.
- Nerikomi: a Japanese method of stacking colored clays to make patterns that run through the wall.
- Marbled clay: two or more clay colors partly wedged together for a swirled look.
Drying terms
Clay passes through set stages as it loses water. Their names tell you what work is possible next.
- Plastic (wet) clay: soft, workable clay straight from the bag or wheel.
- Leather hard: firm enough to hold shape but still damp; the stage for trimming, joining and carving.
- Bone dry: fully air dry, pale and fragile, ready for the bisque firing.
- Greenware: any unfired clay piece, from wet to bone dry.
- Damp box: a closed box that keeps work moist between sessions.
- Ware board: a board for carrying and drying pots.
- Wedging table: a canvas or plaster-topped table for wedging and reclaiming.
- Plaster bat: a plaster slab that pulls water out of wet clay or reclaim.
- S-crack: an S-shaped crack in the base of a thrown pot, usually from an uncompressed floor or uneven drying.
- Warping: a pot bending out of shape as it dries or fires.
- Slaking: letting dry clay soak in water so it breaks down for reclaim.
Glazing and decorating terms
- Glaze: a coating of glass-forming materials that melts onto the pot in the kiln.
- Glazing: applying glaze by dipping, pouring, brushing or spraying.
- Underglaze: colored decorating paint, usually applied under a clear glaze.
- Overglaze: decoration such as china paint, luster or decals fired on top of a glaze at a lower temperature.
- Clear glaze: a transparent glaze that seals and shows the surface beneath.
- Matte glaze: a glaze with a low-shine, non-reflective surface.
- Reactive glaze: a glaze that breaks, flows or varies in color where it is thick or thin.
- Low fire glaze: a glaze made to melt around cone 06 to 04.
- Cone 6 glaze: a mid-fire glaze made to mature at cone 5 to 6.
- Cone 10 glaze: a high-fire glaze for cone 10 kilns.
- Celadon: a clear, often green or blue glaze that pools darker in carved lines.
- Shino: a glaze family known for warm orange to white surfaces.
- Temmoku: an iron glaze that fires glossy black to rust brown.
- Majolica: painted decoration on an opaque white tin or zirconium glaze, usually low fire.
- Crystalline glaze: a glaze that grows visible crystals during a controlled cooling.
- Ash glaze: a glaze made with wood ash.
- Salt glaze: a glaze formed by salt vapor in a hot fuel kiln, with an orange-peel texture.
- Layering: applying one glaze over another for new effects.
- Specific gravity: a measure of how thick a liquid glaze is, used to keep coats consistent.
- Flux: the glaze or clay ingredient that makes others melt at a lower temperature.
- Frit: pre-melted, ground glass used as a glaze ingredient.
- Stain: a manufactured ceramic colorant mixed into glazes, slips or clay.
- Engobe: a slip-like coating that sits between slip and glaze in composition.
- Terra sigillata: a very fine slip brushed on and polished for a soft sheen.
- Burnishing: rubbing leather-hard clay with a smooth tool until it shines.
- Wax resist: wax brushed on to keep glaze off feet or to make patterns.
- Sgraffito: scratching through a colored layer to show the clay below.
- Mishima: carving lines and inlaying them with underglaze or slip.
- Slip trailing: drawing raised lines of slip from a squeeze bottle.
- Decal: a printed transfer fired onto glazed ware.
- Luster: a metallic overglaze fired at low temperature in a third firing.
- Food safe: a maker label for glazes tested for food use when fired as directed; it does not cover how your own pots were glazed and fired.
- Crazing: a fine crack network in fired glaze caused by poor glaze fit.
- Crackle: crazing made on purpose as a decorative effect.
- Crawling: glaze pulling back into beads and leaving bare patches.
- Pinholes: tiny holes in fired glaze from gas escaping the clay or glaze.
- Glaze fit: how well glaze and clay shrink together on cooling.
Firing terms
- Firing: heating clay in a kiln until it turns permanently into ceramic.
- Bisque firing: the first firing that turns greenware into porous, glaze-ready ware.
- Bisqueware: pottery that has had its bisque firing but no glaze yet.
- Glaze firing: the firing that melts glaze onto the pot, also called glost firing.
- Single firing: glazing greenware and firing it once instead of twice.
- Cone: a small ceramic pyramid that bends at a set amount of heat; also the name of the heat level, such as cone 6.
- Cone chart: Orton's table of the temperatures at which each cone bends.
- Heatwork: the combined effect of temperature and time, which is what cones measure.
- Low fire, mid-fire and high fire: rough bands for cone 06 to 04, cone 5 to 6 and cone 10.
- Vitrification: fired clay partly melting into a dense, glassy, less absorbent body.
- Firing schedule: the planned heating rates, temperatures and holds for a firing.
- Ramp: one step in a schedule, given as degrees per hour to a set temperature.
- Hold (soak): keeping the kiln at one temperature for a set time.
- Candling: a slow, low start to dry out the last moisture before a bisque firing.
- Oxidation: firing with plenty of oxygen, as in all electric kilns. See reduction firing.
- Reduction: firing a fuel kiln with limited oxygen, which changes clay and glaze colors.
- Raku: a fast, low firing where glowing pots are pulled out hot and often smoked. See raku pottery.
- Naked raku: a raku method where a resist layer peels away to leave smoke lines on the clay.
- Horsehair raku: laying horsehair on hot unglazed raku ware to burn in fine lines.
- Pit firing: firing pots in a pit or bonfire with combustibles for smoke marks.
- Wood firing: firing with wood, where ash melts into natural glaze; anagama kilns are one type.
- Dunting: cracks from cooling or heating too fast through certain temperatures.
- Bloating: blisters in a clay body from over-firing.
- Thermal shock: cracking from a sudden change in temperature.
Kiln terms
- Kiln: an insulated chamber that fires clay to high temperatures.
- Electric kiln: a kiln heated by coiled elements; the usual home choice.
- Gas kiln: a kiln fired by natural gas or propane that can do reduction.
- Raku kiln: a small, light kiln, often propane, built to open hot.
- Test kiln: a small kiln for tiles, tests and small pieces.
- Front-loading kiln: a kiln with a side door instead of a top lid.
- Microwave kiln: a small insulated cup heated in a microwave, made for glass and metal clay, not pottery.
- 120V and 240V kilns: small kilns that run on household voltage versus larger kilns that need a dedicated 240V circuit; the maker lists the amps and plug. Have a licensed electrician check or install the circuit.
- Controller: the digital unit that runs the firing schedule.
- Digital kiln: a kiln run by a programmable controller.
- Kiln sitter: a mechanical switch that shuts a manual kiln off when a small cone bends.
- Thermocouple: the temperature sensor that reports to the controller.
- Pyrometer: a gauge that shows kiln temperature from a thermocouple.
- Elements: the coiled wires that heat an electric kiln and wear out over time.
- Kiln brick: insulating firebrick that lines the kiln walls.
- Kiln furniture: shelves, posts and stilts that hold ware in the kiln.
- Kiln posts: ceramic columns that hold shelves apart.
- Stilts: small supports for firing glazed-bottom pieces, usually low fire.
- Kiln wash: a coating on shelves that stops glaze drips sticking.
- Kiln vent: a fan system that pulls fumes out of the kiln and room.
- Kiln stand: the metal stand that raises a kiln off the floor.
- Loading: arranging ware on shelves for even heat and safe spacing.
- Saggar: a closed container that protects or smokes ware inside a kiln.
- Kiln maintenance: the cleaning and parts checks set out in the maker's manual.
Tool terms
- Rib: a flat wood, metal, rubber or silicone tool for shaping and smoothing.
- Needle tool: a pointed tool for cutting rims, scoring and checking thickness.
- Fettling knife: a narrow knife for trimming seams and cutting clay.
- Wire cutter: a wire with handles for cutting clay and pots off the wheel.
- Loop tool: a metal loop on a handle for trimming and carving.
- Calipers: a measuring tool for matching lids and widths.
- Sponge: for removing water, smoothing and cleaning.
- Mop brush: a soft round brush that holds a lot of glaze.
- Modeling tools: wood or metal tools for sculpting detail.
- Shaping tools: silicone and rubber tipped tools for pushing and smoothing clay.
- Kanna, tombo and gyubera: Japanese trimming, measuring and shaping tools.
- Texture roller: a patterned roller for pressing texture into slabs.
- Stamp: a carved or molded stamp for marks and makers' chops.
- Slab mat: canvas or a mat that stops clay sticking while you roll.
- Slab cutter: a frame with wires that slices a block into even slabs.
- Clay mixer: a machine that mixes dry clay and water into moist clay.
- Clay trap: a sink fitting that catches clay before it reaches the drain.
- Kiln gloves: heat-resistant gloves for unloading warm ware.
- Pottery apron: a split-leg or full apron for wheel work.
Our pottery tools hub groups every tool guide on the site.
Common mix-ups
- Bisque vs glaze firing: the bisque firing comes first and leaves ware porous; the glaze firing melts the glaze and matures the clay.
- Cone 06 vs cone 6: the zero matters. Cone 06 is low fire; cone 6 is mid-fire and much hotter.
- Underglaze vs glaze: underglaze is mostly color and usually needs clear glaze on top to seal it.
- Kiln vs oven: a kitchen oven cannot fire pottery clay; see pottery oven vs kiln.
Safety words to know: clay and glaze dust contain crystalline silica, so wet clean, never dry sweep, and wear a NIOSH-approved respirator when mixing dry materials. Read the maker's SDS (safety data sheet) for each glaze chemical. Kilns get hot on the outside and need the clearance and ventilation set out in the maker's manual.
What you need
Once the words make sense, the gear list is short: clay matched to your kiln's cone, a basic tool kit and access to a kiln. Our how to start pottery at home guide walks through the first steps, and the best pottery tools guide covers the starter kit.
Sources: AMACO, Laguna Clay and Standard Clay product pages and clay specification sheets (clay body, cone, shrinkage and absorption terms); Orton Ceramic Foundation cone chart and cone product pages (cones, heatwork); Skutt and Paragon kiln operating manuals (controller, thermocouple, elements, kiln sitter, firing schedule terms); Ceramic Arts Network glossary and the Wikipedia glossary of pottery terms (checked for which terms searchers expect, not copied). Checked November 2026.